Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 6.51 g/cm³ Show Material materials with Dichte of 6.51 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 20.0 °C | 14 % Show Material materials with Dehnung A50 of 14 % | |
316.0 °C | 24 % Show Material materials with Dehnung A50 of 24 % | ||
Elastizitätsmodul | 23.0 °C | 68 GPa Show Material materials with Elastizitätsmodul of 68 GPa | Typical for Zirconium |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Zirconium |
Schubmodule | 23.0 °C | 35 GPa Show Material materials with Schubmodule of 35 GPa | Typical for Zirconium |
Streckgrenze Rp 0,2 | 20.0 °C | 240 MPa Show Material materials with Streckgrenze Rp 0,2 of 240 MPa | |
316.0 °C | 105 MPa Show Material materials with Streckgrenze Rp 0,2 of 105 MPa | ||
Zugfestigkeit | 20.0 °C | 415 MPa Show Material materials with Zugfestigkeit of 415 MPa | |
316.0 °C | 215 MPa Show Material materials with Zugfestigkeit of 215 MPa | ||
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.7E-6 - 7E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 5.7E-6 - 7E-6 1/K | Typical for Zirconium |
Schmelzpunkt | 1845 °C Show Material materials with Schmelzpunkt of 1845 °C | Typical for Zirconium | |
Spezifische Wärmekapazität | 23.0 °C | 281 - 289 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 281 - 289 J/(kg·K) | Typical for Zirconium |
Wärmeleitfähigkeit | 23.0 °C | 19 - 27 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 19 - 27 W/(m·K) | Typical for Zirconium |
Chemical properties
Property | Value |
---|---|
Chrom | 0.05 - 0.15 % Show Material materials with Chrom of 0.05 - 0.15 % |
Eisen | 0.07 - 0.2 % Show Material materials with Eisen of 0.07 - 0.2 % |
Nickel | 0.03 - 0.08 % Show Material materials with Nickel of 0.03 - 0.08 % |
Zink | 1.2 - 1.7 % Show Material materials with Zink of 1.2 - 1.7 % |