Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 6.57 g/cm³ Show Material materials with Dichte of 6.57 g/cm³ | Typical for Zirconium |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 20.0 °C | 12 % Show Material materials with Dehnung A50 of 12 % | |
300.0 °C | 12 % Show Material materials with Dehnung A50 of 12 % | ||
Elastizitätsmodul | 23.0 °C | 68 GPa Show Material materials with Elastizitätsmodul of 68 GPa | Typical for Zirconium |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Zirconium |
Schubmodule | 23.0 °C | 35 GPa Show Material materials with Schubmodule of 35 GPa | Typical for Zirconium |
Streckgrenze Rp 0,2 | 20.0 °C | 485 MPa Show Material materials with Streckgrenze Rp 0,2 of 485 MPa | |
300.0 °C | 330 MPa Show Material materials with Streckgrenze Rp 0,2 of 330 MPa | ||
Zugfestigkeit | 20.0 °C | 710 MPa Show Material materials with Zugfestigkeit of 710 MPa | |
300.0 °C | 480 MPa Show Material materials with Zugfestigkeit of 480 MPa | ||
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.7E-6 - 7E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 5.7E-6 - 7E-6 1/K | Typical for Zirconium |
Schmelzpunkt | 1845 °C Show Material materials with Schmelzpunkt of 1845 °C | Typical for Zirconium | |
Spezifische Wärmekapazität | 23.0 °C | 281 - 289 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 281 - 289 J/(kg·K) | Typical for Zirconium |
Wärmeleitfähigkeit | 23.0 °C | 19 - 27 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 19 - 27 W/(m·K) | Typical for Zirconium |
Chemical properties
Property | Value |
---|---|
Niobium | 2.5 - 2.8 % Show Material materials with Niobium of 2.5 - 2.8 % |