Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.57 g/cm³ Show Material materials with Dichte of 8.57 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 20.0 °C | 103 GPa Show Material materials with Elastizitätsmodul of 103 GPa |
Elongation A25 | 20.0 °C | 30 % Show Material materials with Elongation A25 of 30 % |
Härte, Vickers, 10 | 20.0 °C | 60 [-] Show Material materials with Härte, Vickers, 10 of 60 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 50 MPa Show Material materials with Streckgrenze Rp 0,2 of 50 MPa |
Zugfestigkeit | 20.0 °C | 95 MPa Show Material materials with Zugfestigkeit of 95 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Wärmeleitfähigkeit | 20.0 °C | 52 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 52 W/(m·K) |
1000.0 °C | 65 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 65 W/(m·K) | |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 1.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.5E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminium | 5E-3 % Show Material materials with Aluminium of 5E-3 % |
Eisen | 0.01 % Show Material materials with Eisen of 0.01 % |
Hafnium | 0.02 % Show Material materials with Hafnium of 0.02 % |
Kohlenstoff | 0.01 % Show Material materials with Kohlenstoff of 0.01 % |
Molybdän | 0.05 % Show Material materials with Molybdän of 0.05 % |
Nickel | 5E-3 % Show Material materials with Nickel of 5E-3 % |
Sauerstoff | 0.03 % Show Material materials with Sauerstoff of 0.03 % |
Silizium | 5E-3 % Show Material materials with Silizium of 5E-3 % |
Stickstoff | 0.01 % Show Material materials with Stickstoff of 0.01 % |
Tantal | 0.5 % Show Material materials with Tantal of 0.5 % |
Titan | 0.03 % Show Material materials with Titan of 0.03 % |
Wasserstoff | 1.5E-3 % Show Material materials with Wasserstoff of 1.5E-3 % |
Wolfram | 0.05 % Show Material materials with Wolfram of 0.05 % |
Zirkonium | 0.8 - 1.2 % Show Material materials with Zirkonium of 0.8 - 1.2 % |