Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Chrom | 0.05 % Show Material materials with Chrom of 0.05 % |
Eisen | 0.08 % Show Material materials with Eisen of 0.08 % |
Kohlenstoff | 0.025 % Show Material materials with Kohlenstoff of 0.025 % |
Sauerstoff | 0.13 % Show Material materials with Sauerstoff of 0.13 % |
Silizium | 0.05 % Show Material materials with Silizium of 0.05 % |
Stickstoff | 0.02 % Show Material materials with Stickstoff of 0.02 % |
Titan | 0.05 % Show Material materials with Titan of 0.05 % |
Wasserstoff | 5E-3 % Show Material materials with Wasserstoff of 5E-3 % |
Wolfram | 0.02 % Show Material materials with Wolfram of 0.02 % |