Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 19.3 g/cm³ Show Material materials with Dichte of 19.3 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 20.0 °C | 405 - 407 GPa Show Material materials with Elastizitätsmodul of 405 - 407 GPa |
Härte, Vickers | 20.0 °C | 360 [-] Show Material materials with Härte, Vickers of 360 [-] |
Poissonzahl | 20.0 °C | 0.28 [-] Show Material materials with Poissonzahl of 0.28 [-] |
Schubmodule | 20.0 °C | 166 GPa Show Material materials with Schubmodule of 166 GPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4.5E-6 - 4.6E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 4.5E-6 - 4.6E-6 1/K | Typical for Tungsten |
Schmelzpunkt | 3410 °C Show Material materials with Schmelzpunkt of 3410 °C | Typical for Tungsten | |
Spezifische Wärmekapazität | 23.0 °C | 134 - 142 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 134 - 142 J/(kg·K) | Typical for Tungsten |
Wärmeleitfähigkeit | 20.0 °C | 4.2 - 167 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 4.2 - 167 W/(m·K) | |
1000.0 °C | 111 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 111 W/(m·K) | ||
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 5.5E-8 Ω·m Show Material materials with spezifischer Widerstand of 5.5E-8 Ω·m |
1000.0 °C | 3.26E-7 Ω·m Show Material materials with spezifischer Widerstand of 3.26E-7 Ω·m | |
1500.0 °C | 4.86E-7 Ω·m Show Material materials with spezifischer Widerstand of 4.86E-7 Ω·m | |
2000.0 °C | 6.71E-7 Ω·m Show Material materials with spezifischer Widerstand of 6.71E-7 Ω·m | |
Chemical properties
Property | Value |
---|---|
Eisen | 0.01 % Show Material materials with Eisen of 0.01 % |
Kohlenstoff | 0.01 % Show Material materials with Kohlenstoff of 0.01 % |
Nickel | 0.01 % Show Material materials with Nickel of 0.01 % |
Sauerstoff | 0.01 % Show Material materials with Sauerstoff of 0.01 % |
Silizium | 0.01 % Show Material materials with Silizium of 0.01 % |
Stickstoff | 0.01 % Show Material materials with Stickstoff of 0.01 % |
Wolfram | 99.95 % Show Material materials with Wolfram of 99.95 % |