Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 17.15 - 17.85 g/cm³ Show Material materials with Dichte of 17.15 - 17.85 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 2 - 5 % Show Material materials with Dehnung of 2 - 5 % |
Elastizitätsmodul | 20.0 °C | 350 - 360 GPa Show Material materials with Elastizitätsmodul of 350 - 360 GPa |
Härte, Rockwell C | 20.0 °C | 33 [-] Show Material materials with Härte, Rockwell C of 33 [-] |
Schubmodule | 20.0 °C | 135 - 145 GPa Show Material materials with Schubmodule of 135 - 145 GPa |
Streckgrenze Rp 0,2 | 20.0 °C | 517 MPa Show Material materials with Streckgrenze Rp 0,2 of 517 MPa |
Zugfestigkeit | 20.0 °C | 648 - 758 MPa Show Material materials with Zugfestigkeit of 648 - 758 MPa |
Chemical properties
Property | Value |
---|---|
Wolfram | 92.5 % Show Material materials with Wolfram of 92.5 % |