Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 17.75 - 18.35 g/cm³ Show Material materials with Dichte of 17.75 - 18.35 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 1 - 3 % Show Material materials with Dehnung of 1 - 3 % |
Elastizitätsmodul | 20.0 °C | 360 - 380 GPa Show Material materials with Elastizitätsmodul of 360 - 380 GPa |
Härte, Rockwell C | 20.0 °C | 34 [-] Show Material materials with Härte, Rockwell C of 34 [-] |
Schubmodule | 20.0 °C | 140 - 150 GPa Show Material materials with Schubmodule of 140 - 150 GPa |
Streckgrenze Rp 0,2 | 20.0 °C | 517 MPa Show Material materials with Streckgrenze Rp 0,2 of 517 MPa |
Zugfestigkeit | 20.0 °C | 648 - 724 MPa Show Material materials with Zugfestigkeit of 648 - 724 MPa |
Chemical properties
Property | Value |
---|---|
Wolfram | 95 % Show Material materials with Wolfram of 95 % |