Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 18.25 - 18.85 g/cm³ Show Material materials with Dichte of 18.25 - 18.85 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 2 % Show Material materials with Dehnung of 2 % |
Elastizitätsmodul | 20.0 °C | 385 GPa Show Material materials with Elastizitätsmodul of 385 GPa |
Härte, Rockwell C | 20.0 °C | 35 [-] Show Material materials with Härte, Rockwell C of 35 [-] |
Schubmodule | 20.0 °C | 160 GPa Show Material materials with Schubmodule of 160 GPa |
Streckgrenze Rp 0,2 | 20.0 °C | 517 MPa Show Material materials with Streckgrenze Rp 0,2 of 517 MPa |
Zugfestigkeit | 20.0 °C | 689 MPa Show Material materials with Zugfestigkeit of 689 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Wärmeleitfähigkeit | 500.0 °C | 90 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 90 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Wolfram | 97 % Show Material materials with Wolfram of 97 % |