DIN 1725-1 Grade 3.0515 H12

Want to keep this datasheet? Save it now in your required format

Description

The alloy AlMn1 is an Al-Mn alloy, which belongs to the nature-hard aluminum materials. Mn increases the strength compared with pure aluminium, but it does not impair the corrosion resistance. The alloy belongs to the nature-hard aluminum materials. A strength increase can only occur by cold forming. It is very well formable, very well corrosion resistant and weldable. In these characteristics it resembles the pure aluminium, but with the attainable strength it exceeds this. The alloy AlMn1 has a increased heat resistance compared with pure aluminium, as result of the of the Mn-additive (inhibits recrystallisation). Application: In the building industry for roofings, as outer skin of buildings, in the apparatus and tank construction as heat exchanger (bank of tubes, profiles, gilled pipes, sheet metals), for radiators, air conditioning systems, pipings for compressed gas tanks, for tanks according VdTUEV Werkstoffblaetter, as antennas for radio relay link and satellite communication (mirror) for technical flow pressed parts, for solid rivets, for generally metal-describe, in food industry (including commercial devices), in the construction of vehicles (including tank cars) and as packing (sheet metal packings generally).

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM,AluKey zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValueConditionRelated StandardsShape

Dichte

2.73 g/cm³

Show Material materials with Dichte of 2.73 g/cm³

H12

EN 573-3, EN 485

20.0 °C

2.73 g/cm³

Show Material materials with Dichte of 2.73 g/cm³

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Strip

Mechanisch

PropertyTemperatureValueConditionRelated StandardsShapeComment

Biegewinkel 180°

1.5 °/t

Show Material materials with Biegewinkel 180° of 1.5 °/t

H12

EN 573-3, EN 485

Biegewinkel 90°

0.5 °/t

Show Material materials with Biegewinkel 90° of 0.5 °/t

H12

EN 573-3, EN 485

1.0 °/t

Show Material materials with Biegewinkel 90° of 1.0 °/t

H12

EN 573-3, EN 485

2.0 °/t

Show Material materials with Biegewinkel 90° of 2.0 °/t

H12

EN 573-3, EN 485

Dehnung

3.0 %

Show Material materials with Dehnung of 3.0 %

H12

EN 573-3, EN 485

A50

4.0 %

Show Material materials with Dehnung of 4.0 %

H12

EN 573-3, EN 485

A50

5.0 %

Show Material materials with Dehnung of 5.0 %

H12

EN 573-3, EN 485

A50

6.0 %

Show Material materials with Dehnung of 6.0 %

H12

EN 573-3, EN 485

A50

7.0 %

Show Material materials with Dehnung of 7.0 %

H12

EN 573-3, EN 485

A50

8.0 %

Show Material materials with Dehnung of 8.0 %

H12

EN 573-3, EN 485

A100

20.0 °C

5.0 %

Show Material materials with Dehnung of 5.0 %

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Strip

A10

20.0 °C

7.0 %

Show Material materials with Dehnung of 7.0 %

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Strip

20.0 °C

25.0 %

Show Material materials with Dehnung of 25.0 %

H12

DIN 1725-1

Strip

A50 Transverse

Elastizitätsmodul

69.5 GPa

Show Material materials with Elastizitätsmodul of 69.5 GPa

H12

EN 573-3, EN 485

20.0 °C

60.0 - 65.0 GPa

Show Material materials with Elastizitätsmodul of 60.0 - 65.0 GPa

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Strip

Härte, Brinell

36.0 [-]

Show Material materials with Härte, Brinell of 36.0 [-]

H12

EN 573-3, EN 485

20.0 °C

40.0 [-]

Show Material materials with Härte, Brinell of 40.0 [-]

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Strip

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 3000 Series Aluminium

Poissonzahl

0.33 [-]

Show Material materials with Poissonzahl of 0.33 [-]

Typical for Wrought 3000 Series Aluminium

Schubmodule

26.1 GPa

Show Material materials with Schubmodule of 26.1 GPa

H12

EN 573-3, EN 485

20.0 °C

24.0 - 26.5 GPa

Show Material materials with Schubmodule of 24.0 - 26.5 GPa

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Strip

Zugfestigkeit

115.0 - 155.0 MPa

Show Material materials with Zugfestigkeit of 115.0 - 155.0 MPa

H12

EN 573-3, EN 485

20.0 °C

90.0 - 140.0 MPa

Show Material materials with Zugfestigkeit of 90.0 - 140.0 MPa

H12

DIN 1725-1

Strip

Transverse

20.0 °C

120.0 - 160.0 MPa

Show Material materials with Zugfestigkeit of 120.0 - 160.0 MPa

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Strip

Thermisch

PropertyTemperatureValueConditionRelated StandardsShape

Koeffizient der thermischen Ausdehnung

20 °C

2.35e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K

H12

EN 573-3, EN 485

100 °C

2.35e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K

H12

EN 573-3, EN 485

Schmelzpunkt

645.0 - 655.0 °C

Show Material materials with Schmelzpunkt of 645.0 - 655.0 °C

H12

EN 573-3, EN 485

Spezifische Wärmekapazität

893.0 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 893.0 J/(kg·K)

H12

EN 573-3, EN 485

20.0 °C

893.0 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 893.0 J/(kg·K)

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Strip

Wärmeleitfähigkeit

20.0 °C

160.0 - 200.0 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 160.0 - 200.0 W/(m·K)

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4, EN 485

Strip

Elektrisch

PropertyTemperatureValueConditionRelated StandardsShape

Elektrische Leitfähigkeit

20.0 °C

22000000.0 - 28000000.0 S/m

Show Material materials with Elektrische Leitfähigkeit of 22000000.0 - 28000000.0 S/m

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4, EN 485

Strip

spezifischer Widerstand

3.57e-08 - 4.55e-08 Ω·m

Show Material materials with spezifischer Widerstand of 3.57e-08 - 4.55e-08 Ω·m

H12

EN 573-3, EN 485

Chemical properties

PropertyValueConditionRelated StandardsShape

Chrom

0.1 %

Show Material materials with Chrom of 0.1 %

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4, EN 485

Strip

Eisen

0.7 %

Show Material materials with Eisen of 0.7 %

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Strip

0.70 %

Show Material materials with Eisen of 0.70 %

H12

EN 573-3, EN 485

Kupfer

0.1 %

Show Material materials with Kupfer of 0.1 %

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4, EN 485

Strip

Magnesium

0.3 %

Show Material materials with Magnesium of 0.3 %

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4, EN 485

Strip

Mangan

0.9 - 1.5 %

Show Material materials with Mangan of 0.9 - 1.5 %

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4, EN 485

Strip

Silizium

0.5 %

Show Material materials with Silizium of 0.5 %

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4, EN 485

Strip

Titan

0.1

Show Material materials with Titan of 0.1

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4

Strip

Zink

0.2 %

Show Material materials with Zink of 0.2 %

H12

DIN 1725-1, EN 573-3, EN 573-4, VdTÜV WB 513, VdTÜV WB 420-4, EN 485

Strip

Technological properties

Property
Workability

Good workability.