Allgemein
Property | Value | Related Standards | Shape |
---|---|---|---|
Dichte | 2.67 g/cm³ Show Material materials with Dichte of 2.67 g/cm³ | EN 573-3 | Wire, Strip, Sheet, Plate |
Mechanisch
Property | Value | Comment |
---|---|---|
Elastizitätsmodul | 69.0 - 71.0 GPa Show Material materials with Elastizitätsmodul of 69.0 - 71.0 GPa | Typical for Wrought 4000 Series Aluminium |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 4000 Series Aluminium |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 4000 Series Aluminium |
Schubmodule | 26.0 GPa Show Material materials with Schubmodule of 26.0 GPa | Typical for Wrought 4000 Series Aluminium |
Thermisch
Property | Temperature | Value | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.11e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.11e-05 1/K | EN 573-3 | Wire, Strip, Sheet, Plate | |
100 °C | 2.11e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.11e-05 1/K | EN 573-3 | Wire, Strip, Sheet, Plate | ||
Schmelzpunkt | 575.0 - 600.0 °C Show Material materials with Schmelzpunkt of 575.0 - 600.0 °C | EN 573-3 | Wire, Strip, Sheet, Plate | ||
Spezifische Wärmekapazität | 864.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 864.0 J/(kg·K) | Typical for Wrought 4000 Series Aluminium | |||
Wärmeleitfähigkeit | 171 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 171 W/(m·K) | EN 573-3 | Wire, Strip, Sheet, Plate |
Elektrisch
Property | Value | Related Standards | Shape |
---|---|---|---|
Elektrische Leitfähigkeit | 26000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 26000000.0 S/m | EN 573-3 | Wire, Strip, Sheet, Plate |
spezifischer Widerstand | 3.85e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.85e-08 Ω·m | EN 573-3 | Wire, Strip, Sheet, Plate |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Eisen | 0.8 % Show Material materials with Eisen of 0.8 % | EN 573-3 | |
0.80 % Show Material materials with Eisen of 0.80 % | EN 573-3 | Wire, Strip, Sheet, Plate | |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % | EN 573-3 | Wire, Strip, Sheet, Plate |
Magnesium | 0.05 % Show Material materials with Magnesium of 0.05 % | EN 573-3 | Wire, Strip, Sheet, Plate |
Mangan | 0.05 % Show Material materials with Mangan of 0.05 % | EN 573-3 | Wire, Strip, Sheet, Plate |
Silizium | 9.0 - 11.0 % Show Material materials with Silizium of 9.0 - 11.0 % | EN 573-3 | Wire, Strip, Sheet, Plate |
Titan | 0.2 % Show Material materials with Titan of 0.2 % | EN 573-3 | Wire, Strip, Sheet, Plate |
Zink | 0.1 % Show Material materials with Zink of 0.1 % | EN 573-3 | Wire, Strip, Sheet, Plate |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |