Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.66 g/cm³ Show Material materials with Dichte of 2.66 g/cm³ | O3 | EN 573-3, EN 1715-4 | Wire |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastizitätsmodul | 69.0 - 71.0 GPa Show Material materials with Elastizitätsmodul of 69.0 - 71.0 GPa | Typical for Wrought 4000 Series Aluminium | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 4000 Series Aluminium | |||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 4000 Series Aluminium | |||
Schubmodule | 26.0 GPa Show Material materials with Schubmodule of 26.0 GPa | Typical for Wrought 4000 Series Aluminium | |||
Zugfestigkeit | 125.0 - 180.0 MPa Show Material materials with Zugfestigkeit of 125.0 - 180.0 MPa | O3 | EN 573-3, EN 1715-4 | Wire |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.2e-05 - 2.2e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.2e-05 - 2.2e-05 1/K | Typical for Wrought 4000 Series Aluminium |
Schmelzpunkt | 520.0 - 630.0 °C Show Material materials with Schmelzpunkt of 520.0 - 630.0 °C | Typical for Wrought 4000 Series Aluminium |
Spezifische Wärmekapazität | 864.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 864.0 J/(kg·K) | Typical for Wrought 4000 Series Aluminium |
Wärmeleitfähigkeit | 138.0 - 155.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 138.0 - 155.0 W/(m·K) | Typical for Wrought 4000 Series Aluminium |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 23000000.0 - 30000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 23000000.0 - 30000000.0 S/m | Typical for Wrought 4000 Series Aluminium |
spezifischer Widerstand | 3.8e-08 - 5e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.8e-08 - 5e-08 Ω·m | Typical for Wrought 4000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Eisen | 0.60 % Show Material materials with Eisen of 0.60 % | O3 | EN 573-3, EN 1715-4 | Wire |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % | O3 | EN 573-3, EN 1715-4 | Wire |
Magnesium | 0.1 % Show Material materials with Magnesium of 0.1 % | O3 | EN 573-3, EN 1715-4 | Wire |
Mangan | 0.15 % Show Material materials with Mangan of 0.15 % | O3 | EN 573-3, EN 1715-4 | Wire |
Silizium | 11.0 - 13.0 % Show Material materials with Silizium of 11.0 - 13.0 % | O3 | EN 573-3, EN 1715-4 | Wire |
Titan | 0.15 % Show Material materials with Titan of 0.15 % | O3 | EN 573-3, EN 1715-4 | Wire |
Zink | 0.2 % Show Material materials with Zink of 0.2 % | O3 | EN 573-3, EN 1715-4 | Wire |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |