Allgemein
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Dichte | 2.71 g/cm³ Show Material materials with Dichte of 2.71 g/cm³ | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate | |
20.0 °C | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | H24 | EN 573-3 | Flat |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Biegewinkel 180° | 1.5 °/t Show Material materials with Biegewinkel 180° of 1.5 °/t | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
2.0 °/t Show Material materials with Biegewinkel 180° of 2.0 °/t | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
Biegewinkel 90° | 0.5 °/t Show Material materials with Biegewinkel 90° of 0.5 °/t | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
1.0 °/t Show Material materials with Biegewinkel 90° of 1.0 °/t | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
1.5 °/t Show Material materials with Biegewinkel 90° of 1.5 °/t | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate | |||
Elastizitätsmodul | 69.0 - 70.0 GPa Show Material materials with Elastizitätsmodul of 69.0 - 70.0 GPa | Typical for Wrought 5000 Series Aluminium | ||||
Härte, Brinell | 44.0 [-] Show Material materials with Härte, Brinell of 44.0 [-] | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
20.0 °C | 44.0 [-] Show Material materials with Härte, Brinell of 44.0 [-] | H24 | EN 573-3 | Flat | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Schubmodule | 20.0 °C | 27.0 Show Material materials with Schubmodule of 27.0 | H24 | EN 573-3 | Flat | |
Zugfestigkeit | 20.0 °C | 135.0 - 175.0 MPa Show Material materials with Zugfestigkeit of 135.0 - 175.0 MPa | H24 | EN 573-3 | Flat | Transverse |
20.0 °C | 135.0 - 175.0 MPa Show Material materials with Zugfestigkeit of 135.0 - 175.0 MPa | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate, Flat |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.2e-05 - 2.5e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2e-05 - 2.5e-05 1/K | Typical for Wrought 5000 Series Aluminium | ||||
Max. Betriebstemperatur | 150.0 °C Show Material materials with Max. Betriebstemperatur of 150.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Schmelzpunkt | 560.0 - 655.0 °C Show Material materials with Schmelzpunkt of 560.0 - 655.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Spezifische Wärmekapazität | 879.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 879.0 - 963.0 J/(kg·K) | Typical for Wrought 5000 Series Aluminium | ||||
Wärmeleitfähigkeit | 20.0 °C | 215.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 215.0 W/(m·K) | H24 | EN 573-3 | Flat |
Elektrisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 35000000.0 Show Material materials with Elektrische Leitfähigkeit of 35000000.0 | H24 | EN 573-3 | Flat | |
spezifischer Widerstand | 3.3e-08 - 5e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.15 % Show Material materials with Chrom of 0.15 % | H24 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Eisen | 0.7 % Show Material materials with Eisen of 0.7 % | H24 | EN 573-3 | Flat |
0.70 % Show Material materials with Eisen of 0.70 % | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate | |
Kupfer | 0.25 % Show Material materials with Kupfer of 0.25 % | H24 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Magnesium | 0.2 - 0.6 % Show Material materials with Magnesium of 0.2 - 0.6 % | H24 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Mangan | 0.1 - 0.3 % Show Material materials with Mangan of 0.1 - 0.3 % | H24 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % | H24 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Titan | 0.1 % Show Material materials with Titan of 0.1 % | H24 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Zink | 0.3 % Show Material materials with Zink of 0.3 % | H24 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |