Allgemein
Property | Value | Condition | Related Standards |
---|---|---|---|
Dichte | 2.67 g/cm³ Show Material materials with Dichte of 2.67 g/cm³ | H19 | EN 573-3, EN 485, EN 541 |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastizitätsmodul | 69.0 - 70.0 GPa Show Material materials with Elastizitätsmodul of 69.0 - 70.0 GPa | Typical for Wrought 5000 Series Aluminium | ||||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Schubmodule | 26.0 - 26.5 GPa Show Material materials with Schubmodule of 26.0 - 26.5 GPa | Typical for Wrought 5000 Series Aluminium | ||||
Zugfestigkeit | 20.0 °C | 315.0 - 390.0 MPa Show Material materials with Zugfestigkeit of 315.0 - 390.0 MPa | H19 | EN 573-3 | Sheet | |
20.0 °C | 315.0 - 380.0 MPa Show Material materials with Zugfestigkeit of 315.0 - 380.0 MPa | H19 | EN 573-3 | Sheet | ||
20.0 °C | 315.0 - 345.0 MPa Show Material materials with Zugfestigkeit of 315.0 - 345.0 MPa | H19 | EN 573-3 | Sheet | ||
20.0 °C | 340.0 - 380.0 MPa Show Material materials with Zugfestigkeit of 340.0 - 380.0 MPa | H19 | EN 573-3, EN 485, EN 541 | Sheet | ||
20.0 °C | 340.0 - 390.0 MPa Show Material materials with Zugfestigkeit of 340.0 - 390.0 MPa | H19 | EN 573-3 | Sheet | ||
20.0 °C | 340.0 - 345.0 MPa Show Material materials with Zugfestigkeit of 340.0 - 345.0 MPa | H19 | EN 573-3 | Sheet | ||
20.0 °C | 340.0 - 390.0 MPa Show Material materials with Zugfestigkeit of 340.0 - 390.0 MPa | H19 | EN 573-3 | Flat | Transverse | |
20.0 °C | 340.0 - 380.0 MPa Show Material materials with Zugfestigkeit of 340.0 - 380.0 MPa | H19 | EN 573-3 | Flat | Transverse | |
20.0 °C | 345.0 - 350.0 MPa Show Material materials with Zugfestigkeit of 345.0 - 350.0 MPa | H19 | EN 573-3 | Sheet | ||
20.0 °C | 350.0 - 390.0 MPa Show Material materials with Zugfestigkeit of 350.0 - 390.0 MPa | H19 | EN 573-3, EN 485, EN 541 | Sheet | ||
20.0 °C | 350.0 - 380.0 MPa Show Material materials with Zugfestigkeit of 350.0 - 380.0 MPa | H19 | EN 573-3 | Sheet | ||
20.0 °C | 350.0 - 390.0 MPa Show Material materials with Zugfestigkeit of 350.0 - 390.0 MPa | H19 | EN 573-3 | Flat | Transverse | |
20.0 °C | 350.0 - 380.0 MPa Show Material materials with Zugfestigkeit of 350.0 - 380.0 MPa | H19 | EN 573-3 | Flat | Transverse |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.2e-05 - 2.5e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2e-05 - 2.5e-05 1/K | Typical for Wrought 5000 Series Aluminium |
Max. Betriebstemperatur | 150.0 °C Show Material materials with Max. Betriebstemperatur of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Schmelzpunkt | 560.0 - 655.0 °C Show Material materials with Schmelzpunkt of 560.0 - 655.0 °C | Typical for Wrought 5000 Series Aluminium |
Spezifische Wärmekapazität | 879.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 879.0 - 963.0 J/(kg·K) | Typical for Wrought 5000 Series Aluminium |
Wärmeleitfähigkeit | 112.0 - 205.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 112.0 - 205.0 W/(m·K) | Typical for Wrought 5000 Series Aluminium |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 18000000.0 - 31000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 18000000.0 - 31000000.0 S/m | Typical for Wrought 5000 Series Aluminium |
spezifischer Widerstand | 3.3e-08 - 5e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | H19 | EN 573-3, EN 485, EN 541 | Sheet, Flat |
Eisen | 0.35 % Show Material materials with Eisen of 0.35 % | H19 | EN 573-3 | Sheet, Flat |
0.35 % Show Material materials with Eisen of 0.35 % | H19 | EN 573-3, EN 485, EN 541 | ||
Kupfer | 0.15 % Show Material materials with Kupfer of 0.15 % | H19 | EN 573-3, EN 485, EN 541 | Sheet, Flat |
Magnesium | 3.0 - 4.0 % Show Material materials with Magnesium of 3.0 - 4.0 % | H19 | EN 573-3, EN 485, EN 541 | Sheet, Flat |
Mangan | 0.2 - 0.5 % Show Material materials with Mangan of 0.2 - 0.5 % | H19 | EN 573-3, EN 485, EN 541 | Sheet, Flat |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % | H19 | EN 573-3, EN 485, EN 541 | Sheet, Flat |
Titan | 0.1 Show Material materials with Titan of 0.1 | H19 | EN 573-3 | Sheet, Flat |
Zink | 0.25 % Show Material materials with Zink of 0.25 % | H19 | EN 573-3, EN 485, EN 541 | Sheet, Flat |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |