Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 2.7 - 2.71 g/cm³ Show Material materials with Dichte of 2.7 - 2.71 g/cm³ |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 2.00E+7 - 2.50E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 2.00E+7 - 2.50E+7 S/m |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | -270.0 °C | 70 GPa Show Material materials with Elastizitätsmodul of 70 GPa |
20.0 °C | 70 GPa Show Material materials with Elastizitätsmodul of 70 GPa | |
50.0 °C | 69 GPa Show Material materials with Elastizitätsmodul of 69 GPa | |
100.0 °C | 68 GPa Show Material materials with Elastizitätsmodul of 68 GPa | |
150.0 °C | 66 GPa Show Material materials with Elastizitätsmodul of 66 GPa | |
200.0 °C | 63 GPa Show Material materials with Elastizitätsmodul of 63 GPa | |
250.0 °C | 57 GPa Show Material materials with Elastizitätsmodul of 57 GPa | |
300.0 °C | 50 GPa Show Material materials with Elastizitätsmodul of 50 GPa | |
Streckgrenze Rp 0,2 | 20.0 °C | 70 - 80 MPa Show Material materials with Streckgrenze Rp 0,2 of 70 - 80 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Max. Betriebstemperatur, lang | 150 °C Show Material materials with Max. Betriebstemperatur, lang of 150 °C | |
Schmelzpunkt | 650 °C Show Material materials with Schmelzpunkt of 650 °C | |
Wärmeleitfähigkeit | 20.0 °C | 140 - 180 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 140 - 180 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 0.3 % Show Material materials with Chrom of 0.3 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % |
Magnesium | 1.6 - 2.5 % Show Material materials with Magnesium of 1.6 - 2.5 % |
Mangan | 0.5 - 1.1 % Show Material materials with Mangan of 0.5 - 1.1 % |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % |
Titan | 0.1 % Show Material materials with Titan of 0.1 % |
Zink | 0.2 % Show Material materials with Zink of 0.2 % |