Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.75 - 2.84 g/cm³ Show Material materials with Dichte of 2.75 - 2.84 g/cm³ | Typical for Wrought 2000 Series Aluminium |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Dehnung | 20.0 °C | 11.0 % Show Material materials with Dehnung of 11.0 % | F46 | WL 3.1254-1 | |
100.0 °C | 14.0 % Show Material materials with Dehnung of 14.0 % | F46 | WL 3.1254-1 | ||
150.0 °C | 30.0 % Show Material materials with Dehnung of 30.0 % | F46 | WL 3.1254-1 | ||
200.0 °C | 55.0 % Show Material materials with Dehnung of 55.0 % | F46 | WL 3.1254-1 | ||
260.0 °C | 65.0 % Show Material materials with Dehnung of 65.0 % | F46 | WL 3.1254-1 | ||
315.0 °C | 70.0 % Show Material materials with Dehnung of 70.0 % | F46 | WL 3.1254-1 | ||
370.0 °C | 70.0 % Show Material materials with Dehnung of 70.0 % | F46 | WL 3.1254-1 | ||
Elastizitätsmodul | 70.0 - 73.0 GPa Show Material materials with Elastizitätsmodul of 70.0 - 73.0 GPa | Typical for Wrought 2000 Series Aluminium | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | |||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | |||
Schubmodule | 26.0 - 27.5 GPa Show Material materials with Schubmodule of 26.0 - 27.5 GPa | Typical for Wrought 2000 Series Aluminium | |||
Zugfestigkeit | 20.0 °C | 480.0 MPa Show Material materials with Zugfestigkeit of 480.0 MPa | F46 | WL 3.1254-1 | |
100.0 °C | 435.0 MPa Show Material materials with Zugfestigkeit of 435.0 MPa | F46 | WL 3.1254-1 | ||
150.0 °C | 275.0 MPa Show Material materials with Zugfestigkeit of 275.0 MPa | F46 | WL 3.1254-1 | ||
200.0 °C | 110.0 MPa Show Material materials with Zugfestigkeit of 110.0 MPa | F46 | WL 3.1254-1 | ||
260.0 °C | 65.0 MPa Show Material materials with Zugfestigkeit of 65.0 MPa | F46 | WL 3.1254-1 | ||
315.0 °C | 45.0 MPa Show Material materials with Zugfestigkeit of 45.0 MPa | F46 | WL 3.1254-1 | ||
370.0 °C | 30.0 MPa Show Material materials with Zugfestigkeit of 30.0 MPa | F46 | WL 3.1254-1 |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 2.4e-05 1/K | Typical for Wrought 2000 Series Aluminium |
Schmelzpunkt | 500.0 - 650.0 °C Show Material materials with Schmelzpunkt of 500.0 - 650.0 °C | Typical for Wrought 2000 Series Aluminium |
Spezifische Wärmekapazität | 816.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 816.0 - 963.0 J/(kg·K) | Typical for Wrought 2000 Series Aluminium |
Wärmeleitfähigkeit | 112.0 - 251.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 112.0 - 251.0 W/(m·K) | Typical for Wrought 2000 Series Aluminium |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 18000000.0 - 30000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 18000000.0 - 30000000.0 S/m | Typical for Wrought 2000 Series Aluminium |
spezifischer Widerstand | 3.4e-08 - 6e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.4e-08 - 6e-08 Ω·m | Typical for Wrought 2000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Chrom | 0.1 Show Material materials with Chrom of 0.1 | F46 | WL 3.1254-1 |
Eisen | 0.3 Show Material materials with Eisen of 0.3 | F46 | WL 3.1254-1 |
Kupfer | 3.9 - 5.0 % Show Material materials with Kupfer of 3.9 - 5.0 % | F46 | WL 3.1254-1 |
Magnesium | 0.2 - 0.8 % Show Material materials with Magnesium of 0.2 - 0.8 % | F46 | WL 3.1254-1 |
Mangan | 0.4 - 1.2 % Show Material materials with Mangan of 0.4 - 1.2 % | F46 | WL 3.1254-1 |
Silizium | 0.5 - 1.2 % Show Material materials with Silizium of 0.5 - 1.2 % | F46 | WL 3.1254-1 |
Titan | 0.15 Show Material materials with Titan of 0.15 | F46 | WL 3.1254-1 |
Zink | 0.25 Show Material materials with Zink of 0.25 | F46 | WL 3.1254-1 |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |