Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.82 g/cm³ Show Material materials with Dichte of 2.82 g/cm³ | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 9.0 % Show Material materials with Dehnung of 9.0 % | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire | A50 | |
20.0 °C | 9.0 % Show Material materials with Dehnung of 9.0 % | T7452 | WL 3.4394 | Forging | ||
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire | ||
Härte, Brinell | 135.0 [-] Show Material materials with Härte, Brinell of 135.0 [-] | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire | ||
20.0 °C | 135.0 [-] Show Material materials with Härte, Brinell of 135.0 [-] | T7452 | WL 3.4394 | Forging | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | ||||
Schubmodule | 27.0 GPa Show Material materials with Schubmodule of 27.0 GPa | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire | ||
Zugfestigkeit | 480.0 MPa Show Material materials with Zugfestigkeit of 480.0 MPa | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire | ||
490.0 MPa Show Material materials with Zugfestigkeit of 490.0 MPa | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire | |||
495.0 MPa Show Material materials with Zugfestigkeit of 495.0 MPa | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire | |||
20.0 °C | 460.0 MPa Show Material materials with Zugfestigkeit of 460.0 MPa | T7452 | WL 3.4394 | Forging | ||
20.0 °C | 470.0 MPa Show Material materials with Zugfestigkeit of 470.0 MPa | T7452 | WL 3.4394 | Forging | ||
20.0 °C | 475.0 MPa Show Material materials with Zugfestigkeit of 475.0 MPa | T7452 | WL 3.4394 | Forging | ||
20.0 °C | 480.0 MPa Show Material materials with Zugfestigkeit of 480.0 MPa | T7452 | WL 3.4394 | Forging | ||
20.0 °C | 490.0 MPa Show Material materials with Zugfestigkeit of 490.0 MPa | T7452 | WL 3.4394 | Forging | ||
20.0 °C | 495.0 MPa Show Material materials with Zugfestigkeit of 495.0 MPa | T7452 | WL 3.4394 | Forging |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.1e-05 - 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1e-05 - 2.4e-05 1/K | Typical for Wrought 7000 Series Aluminium |
Schmelzpunkt | 465.0 - 655.0 °C Show Material materials with Schmelzpunkt of 465.0 - 655.0 °C | Typical for Wrought 7000 Series Aluminium |
Spezifische Wärmekapazität | 795.0 - 1050.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 795.0 - 1050.0 J/(kg·K) | Typical for Wrought 7000 Series Aluminium |
Wärmeleitfähigkeit | 121.0 - 170.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 121.0 - 170.0 W/(m·K) | Typical for Wrought 7000 Series Aluminium |
Elektrisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Elektrische Leitfähigkeit | 23000000.0 - 25000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 23000000.0 - 25000000.0 S/m | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire |
spezifischer Widerstand | 4e-08 - 4.35e-08 Ω·m Show Material materials with spezifischer Widerstand of 4e-08 - 4.35e-08 Ω·m | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.05 % Show Material materials with Chrom of 0.05 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Eisen | 0.15 % Show Material materials with Eisen of 0.15 % | T7452 | WL 3.4394 | Forging |
0.15 % Show Material materials with Eisen of 0.15 % | T7452 | WL 3.4394 | Sheet, Strip, Bar, Wire | |
Kupfer | 1.5 - 2.0 % Show Material materials with Kupfer of 1.5 - 2.0 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Magnesium | 2.1 - 2.6 % Show Material materials with Magnesium of 2.1 - 2.6 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Nickel | 0.05 % Show Material materials with Nickel of 0.05 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Silizium | 0.12 % Show Material materials with Silizium of 0.12 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Titan | 0.06 % Show Material materials with Titan of 0.06 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Zink | 5.7 - 6.7 % Show Material materials with Zink of 5.7 - 6.7 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Zirkonium | 0.1 - 0.16 % Show Material materials with Zirkonium of 0.1 - 0.16 % | T7452 | WL 3.4394 | Forging, Sheet, Strip, Bar, Wire |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |