Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.8 g/cm³ Show Material materials with Dichte of 2.8 g/cm³ | T4 | EN 573-3, EN 1301, EN 485, EN 754, EN 755 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Bending Fatigue Strength | 140.0 MPa Show Material materials with Bending Fatigue Strength of 140.0 MPa | T4 | EN 573-3, EN 1301, EN 754, EN 755 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | ||
Biegewinkel 90° | 3.0 °/t Show Material materials with Biegewinkel 90° of 3.0 °/t | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | ||
5.0 °/t Show Material materials with Biegewinkel 90° of 5.0 °/t | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | |||
Dehnung | 7.0 % Show Material materials with Dehnung of 7.0 % | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | A100 | |
8.0 % Show Material materials with Dehnung of 8.0 % | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | A100 | ||
10.0 % Show Material materials with Dehnung of 10.0 % | T4 | EN 573-3, EN 754, EN 755 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | A50 | ||
10.0 % Show Material materials with Dehnung of 10.0 % | T4 | EN 573-3, EN 485, EN 755 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | A100 | ||
11.0 % Show Material materials with Dehnung of 11.0 % | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | A50 | ||
11.0 % Show Material materials with Dehnung of 11.0 % | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | A100 | ||
12.0 % Show Material materials with Dehnung of 12.0 % | T4 | EN 573-3, EN 485, EN 754, EN 755 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | A100 | ||
13.0 % Show Material materials with Dehnung of 13.0 % | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | A50 | ||
13.0 % Show Material materials with Dehnung of 13.0 % | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | A100 | ||
14.0 % Show Material materials with Dehnung of 14.0 % | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | A50 | ||
18.0 % Show Material materials with Dehnung of 18.0 % | T4 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | |||
20.0 °C | 7.0 % Show Material materials with Dehnung of 7.0 % | T4 | EN 573-3 | Flat | ||
20.0 °C | 7.0 % Show Material materials with Dehnung of 7.0 % | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 8.0 % Show Material materials with Dehnung of 8.0 % | T4 | EN 573-3 | Rod | ||
20.0 °C | 10.0 % Show Material materials with Dehnung of 10.0 % | T4 | EN 573-3 | Rod, Tube, Profile | A50 | |
20.0 °C | 10.0 % Show Material materials with Dehnung of 10.0 % | T4 | EN 573-3 | Rod, Flat, Profile | ||
20.0 °C | 10.0 % Show Material materials with Dehnung of 10.0 % | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 11.0 % Show Material materials with Dehnung of 11.0 % | T4 | EN 573-3 | Rod | A50 | |
20.0 °C | 11.0 % Show Material materials with Dehnung of 11.0 % | T4 | EN 573-3 | Tube, Profile | ||
20.0 °C | 12.0 % Show Material materials with Dehnung of 12.0 % | T4 | EN 573-3 | Rod, Tube, Flat | ||
20.0 °C | 12.0 % Show Material materials with Dehnung of 12.0 % | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 13.0 % Show Material materials with Dehnung of 13.0 % | T4 | EN 573-3 | Flat | A50 | |
20.0 °C | 13.0 % Show Material materials with Dehnung of 13.0 % | T4 | EN 573-3 | Rod | ||
20.0 °C | 13.0 % Show Material materials with Dehnung of 13.0 % | T4 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 14.0 % Show Material materials with Dehnung of 14.0 % | T4 | EN 573-3 | Flat | A50 | |
20.0 °C | 14.0 % Show Material materials with Dehnung of 14.0 % | T4 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 18.0 % Show Material materials with Dehnung of 18.0 % | T4 | EN 573-3 | Wire | A100 | |
Elastizitätsmodul | 73.0 GPa Show Material materials with Elastizitätsmodul of 73.0 GPa | T4 | EN 573-3, EN 1301, EN 485, EN 754, EN 755 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | ||
Härte, Brinell | 110.0 [-] Show Material materials with Härte, Brinell of 110.0 [-] | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | ||
20.0 °C | 110.0 [-] Show Material materials with Härte, Brinell of 110.0 [-] | T4 | EN 573-3 | Profile, Rod, Flat, Tube | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | ||||
Schubmodule | 27.4 GPa Show Material materials with Schubmodule of 27.4 GPa | T4 | EN 573-3, EN 1301, EN 485, EN 754, EN 755 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | ||
Zugfestigkeit | 350.0 MPa Show Material materials with Zugfestigkeit of 350.0 MPa | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | ||
370.0 MPa Show Material materials with Zugfestigkeit of 370.0 MPa | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | |||
380.0 MPa Show Material materials with Zugfestigkeit of 380.0 MPa | T4 | EN 573-3, EN 1301, EN 754 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | |||
390.0 MPa Show Material materials with Zugfestigkeit of 390.0 MPa | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | |||
395.0 MPa Show Material materials with Zugfestigkeit of 395.0 MPa | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | |||
400.0 MPa Show Material materials with Zugfestigkeit of 400.0 MPa | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | |||
410.0 MPa Show Material materials with Zugfestigkeit of 410.0 MPa | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | |||
20.0 °C | 350.0 MPa Show Material materials with Zugfestigkeit of 350.0 MPa | T4 | EN 573-3 | Rod | ||
20.0 °C | 370.0 MPa Show Material materials with Zugfestigkeit of 370.0 MPa | T4 | EN 573-3 | Rod, Tube, Profile | ||
20.0 °C | 380.0 MPa Show Material materials with Zugfestigkeit of 380.0 MPa | T4 | EN 573-3 | Rod, Tube, Wire | ||
20.0 °C | 390.0 MPa Show Material materials with Zugfestigkeit of 390.0 MPa | T4 | EN 573-3 | Rod | ||
20.0 °C | 395.0 MPa Show Material materials with Zugfestigkeit of 395.0 MPa | T4 | EN 573-3 | Flat | ||
20.0 °C | 395.0 MPa Show Material materials with Zugfestigkeit of 395.0 MPa | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 400.0 MPa Show Material materials with Zugfestigkeit of 400.0 MPa | T4 | EN 573-3 | Flat | ||
20.0 °C | 400.0 MPa Show Material materials with Zugfestigkeit of 400.0 MPa | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 410.0 MPa Show Material materials with Zugfestigkeit of 410.0 MPa | T4 | EN 573-3 | Rod, Profile |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 2.4e-05 1/K | Typical for Wrought 2000 Series Aluminium |
Schmelzpunkt | 500.0 - 650.0 °C Show Material materials with Schmelzpunkt of 500.0 - 650.0 °C | Typical for Wrought 2000 Series Aluminium |
Spezifische Wärmekapazität | 816.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 816.0 - 963.0 J/(kg·K) | Typical for Wrought 2000 Series Aluminium |
Wärmeleitfähigkeit | 112.0 - 251.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 112.0 - 251.0 W/(m·K) | Typical for Wrought 2000 Series Aluminium |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 18000000.0 - 30000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 18000000.0 - 30000000.0 S/m | Typical for Wrought 2000 Series Aluminium |
spezifischer Widerstand | 3.4e-08 - 6e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.4e-08 - 6e-08 Ω·m | Typical for Wrought 2000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Beryllium | 0.0001 - 0.005 % Show Material materials with Beryllium of 0.0001 - 0.005 % | T4 | EN 573-3, EN 1301, EN 485, EN 754, EN 755 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire |
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | T4 | EN 573-3, EN 1301, EN 485, EN 754, EN 755 | Rod, Flat, Tube, Profile, Wire, Strip, Sheet, Plate, Welded Tube |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % | T4 | EN 573-3 | Rod, Flat, Tube, Profile, Wire |
0.50 % Show Material materials with Eisen of 0.50 % | T4 | EN 573-3, EN 1301, EN 485, EN 754, EN 755 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | |
Kupfer | 3.9 - 5.0 % Show Material materials with Kupfer of 3.9 - 5.0 % | T4 | EN 573-3, EN 1301, EN 485, EN 754, EN 755 | Rod, Flat, Tube, Profile, Wire, Strip, Sheet, Plate, Welded Tube |
Magnesium | 0.2 - 0.8 % Show Material materials with Magnesium of 0.2 - 0.8 % | T4 | EN 573-3, EN 1301, EN 485, EN 754, EN 755 | Rod, Flat, Tube, Profile, Wire, Strip, Sheet, Plate, Welded Tube |
Mangan | 0.4 - 1.2 % Show Material materials with Mangan of 0.4 - 1.2 % | T4 | EN 573-3, EN 1301, EN 485, EN 754, EN 755 | Rod, Flat, Tube, Profile, Wire, Strip, Sheet, Plate, Welded Tube |
Nickel | 0.1 % Show Material materials with Nickel of 0.1 % | T4 | EN 573-3, EN 1301, EN 485, EN 754, EN 755 | Rod, Flat, Tube, Profile, Wire, Strip, Sheet, Plate, Welded Tube |
Silizium | 0.5 - 0.9 % Show Material materials with Silizium of 0.5 - 0.9 % | T4 | EN 573-3, EN 1301, EN 485, EN 754, EN 755 | Rod, Flat, Tube, Profile, Wire, Strip, Sheet, Plate, Welded Tube |
Titan | 0.15 % Show Material materials with Titan of 0.15 % | T4 | EN 573-3, EN 1301, EN 485, EN 754, EN 755 | Rod, Flat, Tube, Profile, Wire, Strip, Sheet, Plate, Welded Tube |
Zink | 0.25 % Show Material materials with Zink of 0.25 % | T4 | EN 573-3, EN 1301, EN 485, EN 754, EN 755 | Rod, Flat, Tube, Profile, Wire, Strip, Sheet, Plate, Welded Tube |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |