Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.8 g/cm³ Show Material materials with Dichte of 2.8 g/cm³ | H13 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 5.0 % Show Material materials with Dehnung of 5.0 % | H13 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | ||
Elastizitätsmodul | 73.0 GPa Show Material materials with Elastizitätsmodul of 73.0 GPa | H13 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | ||||
Schubmodule | 27.4 GPa Show Material materials with Schubmodule of 27.4 GPa | H13 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | ||
Zugfestigkeit | 210.0 - 300.0 MPa Show Material materials with Zugfestigkeit of 210.0 - 300.0 MPa | H13 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | ||
20.0 °C | 210.0 MPa Show Material materials with Zugfestigkeit of 210.0 MPa | H13 | EN 573-3 | Wire |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 2.4e-05 1/K | Typical for Wrought 2000 Series Aluminium |
Schmelzpunkt | 500.0 - 650.0 °C Show Material materials with Schmelzpunkt of 500.0 - 650.0 °C | Typical for Wrought 2000 Series Aluminium |
Spezifische Wärmekapazität | 816.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 816.0 - 963.0 J/(kg·K) | Typical for Wrought 2000 Series Aluminium |
Wärmeleitfähigkeit | 112.0 - 251.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 112.0 - 251.0 W/(m·K) | Typical for Wrought 2000 Series Aluminium |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 18000000.0 - 30000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 18000000.0 - 30000000.0 S/m | Typical for Wrought 2000 Series Aluminium |
spezifischer Widerstand | 3.4e-08 - 6e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.4e-08 - 6e-08 Ω·m | Typical for Wrought 2000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Beryllium | 0.0001 - 0.005 % Show Material materials with Beryllium of 0.0001 - 0.005 % | H13 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire |
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | H13 | EN 573-3, EN 1301 | Wire, Strip, Sheet, Plate, Rod, Welded Tube, Tube |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % | H13 | EN 573-3 | Wire |
0.50 % Show Material materials with Eisen of 0.50 % | H13 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | |
Kupfer | 3.9 - 5.0 % Show Material materials with Kupfer of 3.9 - 5.0 % | H13 | EN 573-3, EN 1301 | Wire, Strip, Sheet, Plate, Rod, Welded Tube, Tube |
Magnesium | 0.2 - 0.8 % Show Material materials with Magnesium of 0.2 - 0.8 % | H13 | EN 573-3, EN 1301 | Wire, Strip, Sheet, Plate, Rod, Welded Tube, Tube |
Mangan | 0.4 - 1.2 % Show Material materials with Mangan of 0.4 - 1.2 % | H13 | EN 573-3, EN 1301 | Wire, Strip, Sheet, Plate, Rod, Welded Tube, Tube |
Nickel | 0.1 % Show Material materials with Nickel of 0.1 % | H13 | EN 573-3, EN 1301 | Wire, Strip, Sheet, Plate, Rod, Welded Tube, Tube |
Silizium | 0.5 - 0.9 % Show Material materials with Silizium of 0.5 - 0.9 % | H13 | EN 573-3, EN 1301 | Wire, Strip, Sheet, Plate, Rod, Welded Tube, Tube |
Titan | 0.15 % Show Material materials with Titan of 0.15 % | H13 | EN 573-3, EN 1301 | Wire, Strip, Sheet, Plate, Rod, Welded Tube, Tube |
Zink | 0.25 % Show Material materials with Zink of 0.25 % | H13 | EN 573-3, EN 1301 | Wire, Strip, Sheet, Plate, Rod, Welded Tube, Tube |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |