Allgemein
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Dichte | 20.0 °C | 4.56 g/cm³ Show Material materials with Dichte of 4.56 g/cm³ | Artificially Aged | WL 3.7124-1 | Forging, Rod, Flat |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Dehnung | 20.0 °C | 10.0 % Show Material materials with Dehnung of 10.0 % | Artificially Aged | WL 3.7124-1 | Forging, Rod |
Elastizitätsmodul | 20.0 °C | 113.0 GPa Show Material materials with Elastizitätsmodul of 113.0 GPa | Artificially Aged | WL 3.7124-1 | Forging, Rod, Flat |
Flächenreduzierung | 20.0 °C | 30.0 Show Material materials with Flächenreduzierung of 30.0 | Artificially Aged | WL 3.7124-1 | Forging, Rod |
Zugfestigkeit | 20.0 °C | 650.0 MPa Show Material materials with Zugfestigkeit of 650.0 MPa | Artificially Aged | WL 3.7124-1 | Forging, Rod |
20.0 °C | 690.0 MPa Show Material materials with Zugfestigkeit of 690.0 MPa | Artificially Aged | WL 3.7124-1 | Flat |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 7.599999999999997e-06 - 1.1e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.599999999999997e-06 - 1.1e-05 1/K | Typical for Titanium Alpha Alloy |
Schmelzpunkt | 1540.0 - 1715.0 °C Show Material materials with Schmelzpunkt of 1540.0 - 1715.0 °C | Typical for Titanium Alpha Alloy |
Spezifische Wärmekapazität | 460.0 - 527.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460.0 - 527.0 J/(kg·K) | Typical for Titanium Alpha Alloy |
Wärmeleitfähigkeit | 4.0 - 17.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 4.0 - 17.0 W/(m·K) | Typical for Titanium Alpha Alloy |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Eisen | 0.2 Show Material materials with Eisen of 0.2 | Artificially Aged | WL 3.7124-1 | Forging, Rod, Flat |
Kohlenstoff | 0.1 Show Material materials with Kohlenstoff of 0.1 | Artificially Aged | WL 3.7124-1 | Forging, Rod, Flat |
Kupfer | 2.0 - 3.0 % Show Material materials with Kupfer of 2.0 - 3.0 % | Artificially Aged | WL 3.7124-1 | Forging, Rod, Flat |
Sauerstoff | 0.2 Show Material materials with Sauerstoff of 0.2 | Artificially Aged | WL 3.7124-1 | Forging, Rod, Flat |
Stickstoff | 0.05 Show Material materials with Stickstoff of 0.05 | Artificially Aged | WL 3.7124-1 | Forging, Rod, Flat |
Titan | 96.4 % Show Material materials with Titan of 96.4 % | Artificially Aged | WL 3.7124-1 | Forging, Rod, Flat |
Wasserstoff | 0.01 Show Material materials with Wasserstoff of 0.01 | Artificially Aged | WL 3.7124-1 | Forging, Rod, Flat |