Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 4.506 g/cm³ Show Material materials with Dichte of 4.506 g/cm³ | Typical for Pure Titanium |
Mechanisch
Property | Value | Comment |
---|---|---|
Elastizitätsmodul | 120.0 GPa Show Material materials with Elastizitätsmodul of 120.0 GPa | Typical for Pure Titanium |
Poissonzahl | 0.361 [-] Show Material materials with Poissonzahl of 0.361 [-] | Typical for Pure Titanium |
Schubmodule | 46.0 GPa Show Material materials with Schubmodule of 46.0 GPa | Typical for Pure Titanium |
Thermisch
Property | Temperature | Value | Related Standards | Comment |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium | ||
Schmelzpunkt | 1670.0 °C Show Material materials with Schmelzpunkt of 1670.0 °C | Typical for Pure Titanium | ||
Spezifische Wärmekapazität | 513.0 - 599.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 513.0 - 599.0 J/(kg·K) | Typical for Pure Titanium | ||
Wärmeleitfähigkeit | 20.0 °C | 16.3 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 16.3 W/(m·K) | DIN 17865 |
Elektrisch
Property | Temperature | Value | Related Standards |
---|---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 1750000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 1750000.0 S/m | DIN 17865 |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Eisen | 0.2 Show Material materials with Eisen of 0.2 | DIN 17865 |
Kohlenstoff | 0.1 Show Material materials with Kohlenstoff of 0.1 | DIN 17865 |
Palladium | 0.15 - 0.25 % Show Material materials with Palladium of 0.15 - 0.25 % | DIN 17865 |
Sauerstoff | 0.4 Show Material materials with Sauerstoff of 0.4 | DIN 17865 |
Stickstoff | 0.05 Show Material materials with Stickstoff of 0.05 | DIN 17865 |
Wasserstoff | 0.015 Show Material materials with Wasserstoff of 0.015 | DIN 17865 |