Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 4.506 g/cm³ Show Material materials with Dichte of 4.506 g/cm³ | Typical for Titanium |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Dehnung | 20.0 °C | 5.0 % Show Material materials with Dehnung of 5.0 % | As-Cast | DIN 17865 | |
Elastizitätsmodul | 120.0 GPa Show Material materials with Elastizitätsmodul of 120.0 GPa | Typical for Titanium | |||
Zugfestigkeit | 20.0 °C | 900.0 MPa Show Material materials with Zugfestigkeit of 900.0 MPa | As-Cast | DIN 17865 |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Titanium |
Schmelzpunkt | 1668.0 °C Show Material materials with Schmelzpunkt of 1668.0 °C | Typical for Titanium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminium | 5.7 - 6.3 % Show Material materials with Aluminium of 5.7 - 6.3 % | As-Cast | DIN 17865 |
Eisen | 0.2 Show Material materials with Eisen of 0.2 | As-Cast | DIN 17865 |
Kohlenstoff | 0.1 Show Material materials with Kohlenstoff of 0.1 | As-Cast | DIN 17865 |
Molybdän | 0.25 - 0.75 % Show Material materials with Molybdän of 0.25 - 0.75 % | As-Cast | DIN 17865 |
Sauerstoff | 0.3 Show Material materials with Sauerstoff of 0.3 | As-Cast | DIN 17865 |
Silizium | 0.1 - 0.4 % Show Material materials with Silizium of 0.1 - 0.4 % | As-Cast | DIN 17865 |
Stickstoff | 0.05 Show Material materials with Stickstoff of 0.05 | As-Cast | DIN 17865 |
Wasserstoff | 0.015 Show Material materials with Wasserstoff of 0.015 | As-Cast | DIN 17865 |
Zirkonium | 4.0 - 6.0 % Show Material materials with Zirkonium of 4.0 - 6.0 % | As-Cast | DIN 17865 |
Technological properties
Property | ||
---|---|---|
Processing methods | investment casting, compact casting, separately cast test samples or taken from casting without ingate |