Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 4.506 g/cm³ Show Material materials with Dichte of 4.506 g/cm³ | Typical for Titanium |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Dehnung | 20.0 °C | 5.0 % Show Material materials with Dehnung of 5.0 % | Annealed | WL 3.7264-1, DIN 17865 | |
Elastizitätsmodul | 120.0 GPa Show Material materials with Elastizitätsmodul of 120.0 GPa | Typical for Titanium | |||
Flächenreduzierung | 20.0 °C | 10.0 % Show Material materials with Flächenreduzierung of 10.0 % | Annealed | WL 3.7264-1, DIN 17865 | |
Zugfestigkeit | 20.0 °C | 880.0 MPa Show Material materials with Zugfestigkeit of 880.0 MPa | Annealed | WL 3.7264-1, DIN 17865 |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Titanium | |||
Schmelzpunkt | 1668.0 °C Show Material materials with Schmelzpunkt of 1668.0 °C | Typical for Titanium | |||
Wärmeleitfähigkeit | 20.0 °C | 7.1 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 7.1 W/(m·K) | Annealed | WL 3.7264-1, DIN 17865 |
Elektrisch
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 580000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 580000.0 S/m | Annealed | WL 3.7264-1, DIN 17865 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminium | 5.5 - 6.7 % Show Material materials with Aluminium of 5.5 - 6.7 % | Annealed | WL 3.7264-1, DIN 17865 |
Eisen | 0.3 Show Material materials with Eisen of 0.3 | Annealed | WL 3.7264-1, DIN 17865 |
Kohlenstoff | 0.1 Show Material materials with Kohlenstoff of 0.1 | Annealed | WL 3.7264-1, DIN 17865 |
Sauerstoff | 0.25 Show Material materials with Sauerstoff of 0.25 | Annealed | WL 3.7264-1, DIN 17865 |
Stickstoff | 0.05 Show Material materials with Stickstoff of 0.05 | Annealed | WL 3.7264-1, DIN 17865 |
Titan | 87.7 % Show Material materials with Titan of 87.7 % | Annealed | WL 3.7264-1, DIN 17865 |
Vanadium | 3.5 - 4.5 % Show Material materials with Vanadium of 3.5 - 4.5 % | Annealed | WL 3.7264-1, DIN 17865 |
Wasserstoff | 0.015 Show Material materials with Wasserstoff of 0.015 | Annealed | WL 3.7264-1, DIN 17865 |
Technological properties
Property | ||
---|---|---|
Processing methods | investment casting, sample taken from casting or separately cast or cast on |