Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 5 g/cm³ Show Material materials with Dichte of 5 g/cm³ | Typical for Zinc Aluminium |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation A10 | 20.0 °C | 60 - 80 % Show Material materials with Elongation A10 of 60 - 80 % | |
Härte, Brinell | 20.0 °C | 40 - 50 [-] Show Material materials with Härte, Brinell of 40 - 50 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Zinc Aluminium |
Zugfestigkeit | 20.0 °C | 200 - 240 MPa Show Material materials with Zugfestigkeit of 200 - 240 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc Aluminium |
Schmelzpunkt | 375 - 485 °C Show Material materials with Schmelzpunkt of 375 - 485 °C | Typical for Zinc Aluminium | |
Spezifische Wärmekapazität | 23.0 °C | 393 - 525 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 393 - 525 J/(kg·K) | Typical for Zinc Aluminium |
Wärmeleitfähigkeit | 23.0 °C | 105 - 125 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 105 - 125 W/(m·K) | Typical for Zinc Aluminium |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.7 - 0.9 % Show Material materials with Aluminium of 0.7 - 0.9 % |
Kupfer | 0.3 - 0.5 % Show Material materials with Kupfer of 0.3 - 0.5 % |
Zink | 98.6 % Show Material materials with Zink of 98.6 % |