Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 11.34 g/cm³ Show Material materials with Dichte of 11.34 g/cm³ | Typical for Pure/Low Alloyed Lead |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Poissonzahl | 23.0 °C | 0.4 [-] Show Material materials with Poissonzahl of 0.4 [-] | Typical for Pure/Low Alloyed Lead |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 327 °C Show Material materials with Schmelzpunkt of 327 °C | Typical for Pure/Low Alloyed Lead | |
Spezifische Wärmekapazität | 23.0 °C | 112 - 134 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 112 - 134 J/(kg·K) | Typical for Pure/Low Alloyed Lead |
Wärmeleitfähigkeit | 23.0 °C | 34 - 35 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 34 - 35 W/(m·K) | Typical for Pure/Low Alloyed Lead |
Chemical properties
Property | Value |
---|---|
Antimon | 1E-3 % Show Material materials with Antimon of 1E-3 % |
Arsen | 1E-3 % Show Material materials with Arsen of 1E-3 % |
Bismut | 0.027 % Show Material materials with Bismut of 0.027 % |
Blei | 99.97 % Show Material materials with Blei of 99.97 % |
Eisen | 1E-3 % Show Material materials with Eisen of 1E-3 % |
Kupfer | 1E-3 % Show Material materials with Kupfer of 1E-3 % |
Silber | 3E-3 % Show Material materials with Silber of 3E-3 % |
Zink | 1E-3 % Show Material materials with Zink of 1E-3 % |
Zinn | 1E-3 % Show Material materials with Zinn of 1E-3 % |