Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 11.34 g/cm³ Show Material materials with Dichte of 11.34 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 20.0 °C | 17 GPa Show Material materials with Elastizitätsmodul of 17 GPa | |
Härte, Brinell | 20.0 °C | 3.3 - 4.7 [-] Show Material materials with Härte, Brinell of 3.3 - 4.7 [-] | |
Härte, Vickers | 20.0 °C | 3.2 - 4.7 [-] Show Material materials with Härte, Vickers of 3.2 - 4.7 [-] | |
Poissonzahl | 23.0 °C | 0.4 [-] Show Material materials with Poissonzahl of 0.4 [-] | Typical for Pure/Low Alloyed Lead |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 327 °C Show Material materials with Schmelzpunkt of 327 °C | Typical for Pure/Low Alloyed Lead | |
Spezifische Wärmekapazität | 23.0 °C | 112 - 134 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 112 - 134 J/(kg·K) | Typical for Pure/Low Alloyed Lead |
Wärmeleitfähigkeit | 23.0 °C | 34 - 35 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 34 - 35 W/(m·K) | Typical for Pure/Low Alloyed Lead |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 2.07E-7 Ω·m Show Material materials with spezifischer Widerstand of 2.07E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Antimon | 1E-3 % Show Material materials with Antimon of 1E-3 % |
Arsen | 1E-3 % Show Material materials with Arsen of 1E-3 % |
Bismut | 0.05 % Show Material materials with Bismut of 0.05 % |
Blei | 99.94 % Show Material materials with Blei of 99.94 % |
Eisen | 1E-3 % Show Material materials with Eisen of 1E-3 % |
Kupfer | 0.03 - 0.05 % Show Material materials with Kupfer of 0.03 - 0.05 % |
Silber | 5E-3 % Show Material materials with Silber of 5E-3 % |
Zink | 1E-3 % Show Material materials with Zink of 1E-3 % |
Zinn | 5E-3 % Show Material materials with Zinn of 5E-3 % |