Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 9.6 g/cm³ Show Material materials with Dichte of 9.6 g/cm³ | Typical for Lead Antimony |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 235 - 305 °C Show Material materials with Schmelzpunkt of 235 - 305 °C | Typical for Lead Antimony | |
Spezifische Wärmekapazität | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Wärmeleitfähigkeit | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Antimon | 0.75 - 1.25 % Show Material materials with Antimon of 0.75 - 1.25 % |
Arsen | 0.02 - 0.05 % Show Material materials with Arsen of 0.02 - 0.05 % |
Blei | 98.7 % Show Material materials with Blei of 98.7 % |