Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 11.34 g/cm³ Show Material materials with Dichte of 11.34 g/cm³ | Typical for Pure/Low Alloyed Lead |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Poissonzahl | 23.0 °C | 0.4 [-] Show Material materials with Poissonzahl of 0.4 [-] | Typical for Pure/Low Alloyed Lead |
Zugfestigkeit | 20.0 °C | 15 - 30 MPa Show Material materials with Zugfestigkeit of 15 - 30 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 327 °C Show Material materials with Schmelzpunkt of 327 °C | Typical for Pure/Low Alloyed Lead | |
Spezifische Wärmekapazität | 23.0 °C | 112 - 134 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 112 - 134 J/(kg·K) | Typical for Pure/Low Alloyed Lead |
Wärmeleitfähigkeit | 23.0 °C | 34 - 35 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 34 - 35 W/(m·K) | Typical for Pure/Low Alloyed Lead |
Chemical properties
Property | Value |
---|---|
Antimon | 0.2 - 0.3 % Show Material materials with Antimon of 0.2 - 0.3 % |
Blei | 99.7 % Show Material materials with Blei of 99.7 % |