Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 9.6 g/cm³ Show Material materials with Dichte of 9.6 g/cm³ | Typical for Lead Antimony |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 235 - 305 °C Show Material materials with Schmelzpunkt of 235 - 305 °C | Typical for Lead Antimony | |
Spezifische Wärmekapazität | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Wärmeleitfähigkeit | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Antimon | 0.5 - 0.6 % Show Material materials with Antimon of 0.5 - 0.6 % |
Arsen | 5E-3 % Show Material materials with Arsen of 5E-3 % |
Bismut | 0.05 % Show Material materials with Bismut of 0.05 % |
Blei | 99.33 % Show Material materials with Blei of 99.33 % |
Cadmium | 1E-3 % Show Material materials with Cadmium of 1E-3 % |
Kupfer | 3E-3 % Show Material materials with Kupfer of 3E-3 % |
Nickel | 1E-3 % Show Material materials with Nickel of 1E-3 % |
Silber | 5E-3 % Show Material materials with Silber of 5E-3 % |
Tellur | 2E-3 % Show Material materials with Tellur of 2E-3 % |
Zink | 1E-3 % Show Material materials with Zink of 1E-3 % |
Zinn | 5E-3 % Show Material materials with Zinn of 5E-3 % |