Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 185 - 320 °C Show Material materials with Schmelzpunkt of 185 - 320 °C | Typical for Lead Tin | |
Spezifische Wärmekapazität | 23.0 °C | 213 - 239 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 213 - 239 J/(kg·K) | Typical for Lead Tin |
Wärmeleitfähigkeit | 23.0 °C | 35 - 57 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 35 - 57 W/(m·K) | Typical for Lead Tin |
Chemical properties
Property | Value |
---|---|
Antimon | 0.06 - 0.1 % Show Material materials with Antimon of 0.06 - 0.1 % |
Arsen | 1E-3 % Show Material materials with Arsen of 1E-3 % |
Bismut | 0.03 % Show Material materials with Bismut of 0.03 % |
Blei | 99.41 % Show Material materials with Blei of 99.41 % |
Cadmium | 1E-3 % Show Material materials with Cadmium of 1E-3 % |
Kupfer | 3E-3 % Show Material materials with Kupfer of 3E-3 % |
Nickel | 1E-3 % Show Material materials with Nickel of 1E-3 % |
Silber | 5E-3 % Show Material materials with Silber of 5E-3 % |
Tellur | 2E-3 % Show Material materials with Tellur of 2E-3 % |
Zink | 1E-3 % Show Material materials with Zink of 1E-3 % |
Zinn | 0.35 - 0.45 % Show Material materials with Zinn of 0.35 - 0.45 % |