Allgemein
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Dichte | 20.0 °C | 2.65 g/cm³ Show Material materials with Dichte of 2.65 g/cm³ | F | DIN 1725-2, EN 1676, EN 1706 |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Dehnung | 20.0 °C | 1.0 - 3.0 % Show Material materials with Dehnung of 1.0 - 3.0 % | F | DIN 1725-2, EN 1676, EN 1706 | |
Elastizitätsmodul | 20.0 °C | 74.0 GPa Show Material materials with Elastizitätsmodul of 74.0 GPa | F | DIN 1725-2, EN 1676, EN 1706 | |
Härte, Brinell | 20.0 °C | 70.0 - 100.0 [-] Show Material materials with Härte, Brinell of 70.0 - 100.0 [-] | F | DIN 1725-2, EN 1676, EN 1706 | |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | |||
Scherfestigkeit | 20.0 °C | 147.0 MPa Show Material materials with Scherfestigkeit of 147.0 MPa | F | DIN 1725-2, EN 1676, EN 1706 | |
Schubmodule | 2.8 GPa Show Material materials with Schubmodule of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | |||
Zugfestigkeit | 20.0 °C | 220.0 - 300.0 MPa Show Material materials with Zugfestigkeit of 220.0 - 300.0 MPa | F | DIN 1725-2, EN 1676, EN 1706 |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 200.0 °C | 2.1e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1e-05 1/K | F | DIN 1725-2, EN 1676, EN 1706 | |
Schmelzpunkt | 505.0 - 770.0 °C Show Material materials with Schmelzpunkt of 505.0 - 770.0 °C | Typical for Cast 3xx.x Series Aluminium | |||
Spezifische Wärmekapazität | 20.0 °C | 910.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 910.0 J/(kg·K) | F | DIN 1725-2, EN 1676, EN 1706 | |
Wärmeleitfähigkeit | 20.0 °C | 120.0 - 150.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 120.0 - 150.0 W/(m·K) | F | DIN 1725-2, EN 1676, EN 1706 |
Elektrisch
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 16000000.0 - 20000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 16000000.0 - 20000000.0 S/m | F | DIN 1725-2, EN 1676, EN 1706 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminium | 86.6 % Show Material materials with Aluminium of 86.6 % | F | DIN 1725-2, EN 1676, EN 1706 |
Eisen | 1.0 Show Material materials with Eisen of 1.0 | F | DIN 1725-2, EN 1676, EN 1706 |
Kupfer | 0.1 Show Material materials with Kupfer of 0.1 | F | DIN 1725-2, EN 1676, EN 1706 |
Magnesium | 0.2 - 0.5 % Show Material materials with Magnesium of 0.2 - 0.5 % | F | DIN 1725-2, EN 1676, EN 1706 |
Mangan | 0.001 - 0.4 % Show Material materials with Mangan of 0.001 - 0.4 % | F | DIN 1725-2, EN 1676, EN 1706 |
Silizium | 9.0 - 11.0 % Show Material materials with Silizium of 9.0 - 11.0 % | F | DIN 1725-2, EN 1676, EN 1706 |
Titan | 0.15 Show Material materials with Titan of 0.15 | F | DIN 1725-2, EN 1676, EN 1706 |
Zink | 0.1 Show Material materials with Zink of 0.1 | F | DIN 1725-2, EN 1676, EN 1706 |
Technological properties
Property | ||
---|---|---|
Processing methods | pressure die casting, separately cast test sample |