Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 6.7 g/cm³ Show Material materials with Dichte of 6.7 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 2 - 5 % Show Material materials with Dehnung of 2 - 5 % | |
Elastizitätsmodul | 20.0 °C | 130 GPa Show Material materials with Elastizitätsmodul of 130 GPa | |
Härte, Brinell | 20.0 °C | 85 - 105 [-] Show Material materials with Härte, Brinell of 85 - 105 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Zinc Aluminium |
Streckgrenze Rp 0,2 | 20.0 °C | 220 - 250 MPa Show Material materials with Streckgrenze Rp 0,2 of 220 - 250 MPa | |
Zugfestigkeit | 20.0 °C | 280 - 350 MPa Show Material materials with Zugfestigkeit of 280 - 350 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc Aluminium |
Schmelzpunkt | 375 - 485 °C Show Material materials with Schmelzpunkt of 375 - 485 °C | Typical for Zinc Aluminium | |
Spezifische Wärmekapazität | 20.0 °C | 427 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 427 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 92 - 100 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 92 - 100 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 1.60E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 1.60E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | 3.5 - 4.3 % Show Material materials with Aluminium of 3.5 - 4.3 % |
Eisen | 5E-3 % Show Material materials with Eisen of 5E-3 % |
Kupfer | 0.4 - 1.1 % Show Material materials with Kupfer of 0.4 - 1.1 % |
Magnesium | 0.02 - 0.06 % Show Material materials with Magnesium of 0.02 - 0.06 % |
Nickel | 0.02 % Show Material materials with Nickel of 0.02 % |
Zink | 94.44 % Show Material materials with Zink of 94.44 % |
Zinn | 0.02 % Show Material materials with Zinn of 0.02 % |
Technological properties
Property | ||
---|---|---|
Processing methods | pressure die casting, separately cast test sample |