Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 5 g/cm³ Show Material materials with Dichte of 5 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 20.0 °C | 3 - 6 % Show Material materials with Dehnung A50 of 3 - 6 % | |
Elastizitätsmodul | 20.0 °C | 75 GPa Show Material materials with Elastizitätsmodul of 75 GPa | |
Härte, Brinell | 20.0 °C | 110 - 120 [-] Show Material materials with Härte, Brinell of 110 - 120 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Zinc Aluminium |
Streckgrenze Rp 0,2 | 20.0 °C | 338 - 345 MPa Show Material materials with Streckgrenze Rp 0,2 of 338 - 345 MPa | |
Zugfestigkeit | 20.0 °C | 400 - 440 MPa Show Material materials with Zugfestigkeit of 400 - 440 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc Aluminium |
Schmelzpunkt | 375 - 485 °C Show Material materials with Schmelzpunkt of 375 - 485 °C | Typical for Zinc Aluminium | |
Spezifische Wärmekapazität | 23.0 °C | 393 - 525 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 393 - 525 J/(kg·K) | Typical for Zinc Aluminium |
Wärmeleitfähigkeit | 23.0 °C | 105 - 125 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 105 - 125 W/(m·K) | Typical for Zinc Aluminium |
Chemical properties
Property | Value |
---|---|
Aluminium | 25 - 28 % Show Material materials with Aluminium of 25 - 28 % |
Blei | 4E-3 % Show Material materials with Blei of 4E-3 % |
Cadmium | 3E-3 % Show Material materials with Cadmium of 3E-3 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Kupfer | 2 - 2.5 % Show Material materials with Kupfer of 2 - 2.5 % |
Magnesium | 0.01 - 0.02 % Show Material materials with Magnesium of 0.01 - 0.02 % |
Zink | 69.37 % Show Material materials with Zink of 69.37 % |
Zinn | 2E-3 % Show Material materials with Zinn of 2E-3 % |
Technological properties
Property | ||
---|---|---|
Processing methods | sand casting |