Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 6.3 g/cm³ Show Material materials with Dichte of 6.3 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 20.0 °C | 1 - 2 % Show Material materials with Dehnung A50 of 1 - 2 % | |
Elastizitätsmodul | 20.0 °C | 85 GPa Show Material materials with Elastizitätsmodul of 85 GPa | |
Härte, Brinell | 20.0 °C | 85 - 90 [-] Show Material materials with Härte, Brinell of 85 - 90 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Zinc Aluminium |
Streckgrenze Rp 0,2 | 20.0 °C | 190 - 200 MPa Show Material materials with Streckgrenze Rp 0,2 of 190 - 200 MPa | |
Zugfestigkeit | 20.0 °C | 220 - 275 MPa Show Material materials with Zugfestigkeit of 220 - 275 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc Aluminium |
Schmelzpunkt | 375 - 485 °C Show Material materials with Schmelzpunkt of 375 - 485 °C | Typical for Zinc Aluminium | |
Spezifische Wärmekapazität | 23.0 °C | 393 - 525 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 393 - 525 J/(kg·K) | Typical for Zinc Aluminium |
Wärmeleitfähigkeit | 23.0 °C | 105 - 125 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 105 - 125 W/(m·K) | Typical for Zinc Aluminium |
Chemical properties
Property | Value |
---|---|
Aluminium | 8 - 8.8 % Show Material materials with Aluminium of 8 - 8.8 % |
Blei | 4E-3 % Show Material materials with Blei of 4E-3 % |
Cadmium | 3E-3 % Show Material materials with Cadmium of 3E-3 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Kupfer | 0.8 - 1.3 % Show Material materials with Kupfer of 0.8 - 1.3 % |
Magnesium | 0.02 - 0.03 % Show Material materials with Magnesium of 0.02 - 0.03 % |
Zink | 89.76 % Show Material materials with Zink of 89.76 % |
Zinn | 2E-3 % Show Material materials with Zinn of 2E-3 % |
Technological properties
Property | ||
---|---|---|
Processing methods | permanent mould casting |