Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 10.4 g/cm³ Show Material materials with Dichte of 10.4 g/cm³ |
Mechanisch
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 235 - 305 °C Show Material materials with Schmelzpunkt of 235 - 305 °C | Typical for Lead Antimony | |
Spezifische Wärmekapazität | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Wärmeleitfähigkeit | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Antimon | 14.5 - 15.5 % Show Material materials with Antimon of 14.5 - 15.5 % |
Arsen | 0.05 % Show Material materials with Arsen of 0.05 % |
Blei | 79 - 81 % Show Material materials with Blei of 79 - 81 % |
Cadmium | 0.05 % Show Material materials with Cadmium of 0.05 % |
Eisen | 0.05 % Show Material materials with Eisen of 0.05 % |
Zinn | 4.5 - 5.5 % Show Material materials with Zinn of 4.5 - 5.5 % |
Technological properties
Property | ||
---|---|---|
Processing methods | pressure die casting, separately cast test sample,pressure die casting |