Allgemein
Property | Value | Related Standards | Shape |
---|---|---|---|
Dichte | 2.705 g/cm³ Show Material materials with Dichte of 2.705 g/cm³ | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Mechanisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Elastizitätsmodul | 69.0 GPa Show Material materials with Elastizitätsmodul of 69.0 GPa | EN 573-3 | Strip, Sheet, Plate, Tube, Bar | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | ||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | ||
Schubmodule | 25.9 GPa Show Material materials with Schubmodule of 25.9 GPa | Typical for Wrought 1000 Series Aluminium |
Thermisch
Property | Temperature | Value | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.36e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K | EN 573-3 | Strip, Sheet, Plate, Tube, Bar | |
100 °C | 2.36e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K | EN 573-3 | Strip, Sheet, Plate, Tube, Bar | ||
Schmelzpunkt | 645.0 - 655.0 °C Show Material materials with Schmelzpunkt of 645.0 - 655.0 °C | EN 573-3 | Strip, Sheet, Plate, Tube, Bar | ||
Spezifische Wärmekapazität | 900.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 900.0 - 963.0 J/(kg·K) | Typical for Wrought 1000 Series Aluminium | |||
Wärmeleitfähigkeit | 230.0 - 234.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 230.0 - 234.0 W/(m·K) | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Elektrisch
Property | Value | Related Standards | Shape |
---|---|---|---|
Elektrische Leitfähigkeit | 35000000.0 - 36000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 35000000.0 - 36000000.0 S/m | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
spezifischer Widerstand | 2.78e-08 - 2.86e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.78e-08 - 2.86e-08 Ω·m | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 99.6 % Show Material materials with Aluminium of 99.6 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Eisen | 0.35 % Show Material materials with Eisen of 0.35 % | EN 573-3 | |
0.35 % Show Material materials with Eisen of 0.35 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar | |
Kupfer | 0.05 % Show Material materials with Kupfer of 0.05 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Magnesium | 0.03 % Show Material materials with Magnesium of 0.03 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Mangan | 0.03 % Show Material materials with Mangan of 0.03 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Silizium | 0.25 % Show Material materials with Silizium of 0.25 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Titan | 0.03 % Show Material materials with Titan of 0.03 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Vanadium | 0.05 % Show Material materials with Vanadium of 0.05 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Zink | 0.05 % Show Material materials with Zink of 0.05 % | EN 573-3 | Strip, Sheet, Plate, Tube, Bar |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |