Allgemein
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 25.0 % Show Material materials with Dehnung of 25.0 % | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | ||
29.0 % Show Material materials with Dehnung of 29.0 % | O | EN 573-3 | Strip, Sheet, Plate | |||
30.0 % Show Material materials with Dehnung of 30.0 % | O | EN 573-3 | Strip, Sheet, Plate | |||
33.0 % Show Material materials with Dehnung of 33.0 % | O | EN 573-3 | Strip, Sheet, Plate | |||
20.0 °C | 25.0 % Show Material materials with Dehnung of 25.0 % | O | EN 573-3 | Wire | A100 | |
20.0 °C | 29.0 % Show Material materials with Dehnung of 29.0 % | O | EN 573-3 | Rod | ||
20.0 °C | 30.0 % Show Material materials with Dehnung of 30.0 % | O | EN 573-3 | Sheet, Strip | ||
20.0 °C | 33.0 % Show Material materials with Dehnung of 33.0 % | O | EN 573-3 | Sheet, Strip | ||
Elastizitätsmodul | -270 °C | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | O | EN 573-3 | Strip, Sheet, Plate, Wire, Rod | |
-270.0 °C | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | O | EN 573-3 | Strip, Sheet, Plate, Wire, Rod | ||
70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | |||
20 °C | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | O | EN 573-3 | Strip, Sheet, Plate, Wire, Rod | ||
20.0 °C | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | O | EN 573-3 | Strip, Sheet, Plate, Wire, Rod | ||
20.0 °C | 70.0 - 72.0 GPa Show Material materials with Elastizitätsmodul of 70.0 - 72.0 GPa | O | EN 573-3 | Wire, Rod, Sheet, Strip | ||
20.0 °C | 72.0 GPa Show Material materials with Elastizitätsmodul of 72.0 GPa | O | EN 573-3 | Wire | ||
50.0 °C | 69.0 GPa Show Material materials with Elastizitätsmodul of 69.0 GPa | O | EN 573-3 | Wire, Rod, Sheet, Strip | ||
100.0 °C | 68.0 GPa Show Material materials with Elastizitätsmodul of 68.0 GPa | O | EN 573-3 | Wire, Rod, Sheet, Strip | ||
150.0 °C | 66.0 GPa Show Material materials with Elastizitätsmodul of 66.0 GPa | O | EN 573-3 | Wire, Rod, Sheet, Strip | ||
200.0 °C | 63.0 GPa Show Material materials with Elastizitätsmodul of 63.0 GPa | O | EN 573-3 | Wire, Rod, Sheet, Strip | ||
250.0 °C | 57.0 GPa Show Material materials with Elastizitätsmodul of 57.0 GPa | O | EN 573-3 | Wire, Rod, Sheet, Strip | ||
300 °C | 50.0 GPa Show Material materials with Elastizitätsmodul of 50.0 GPa | O | EN 573-3 | Strip, Sheet, Plate, Wire, Rod | ||
300.0 °C | 50.0 GPa Show Material materials with Elastizitätsmodul of 50.0 GPa | O | EN 573-3 | Strip, Sheet, Plate, Wire, Rod | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | ||||
Schubmodule | 20.0 °C | 25.0 - 26.5 GPa Show Material materials with Schubmodule of 25.0 - 26.5 GPa | O | EN 573-3 | Rod, Sheet, Strip, Wire | |
Zugfestigkeit | 40.0 MPa Show Material materials with Zugfestigkeit of 40.0 MPa | O | EN 573-3 | Strip, Sheet, Plate | ||
70.0 MPa Show Material materials with Zugfestigkeit of 70.0 MPa | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | |||
20.0 °C | 40.0 MPa Show Material materials with Zugfestigkeit of 40.0 MPa | O | EN 573-3 | Rod, Sheet, Strip | ||
20.0 °C | 70.0 MPa Show Material materials with Zugfestigkeit of 70.0 MPa | O | EN 573-3 | Wire |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | -50 °C | 2.18e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.18e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire |
-50.0 °C | 2.18e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.18e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire | |
20 °C | 2.18e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.18e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire | |
20 °C | 2.35e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | |
20 °C | 2.45e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.45e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire | |
20 °C | 2.55e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.55e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire | |
100 °C | 2.35e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | |
100.0 °C | 2.36e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K | O | EN 573-3 | Rod, Sheet, Strip, Wire | |
200 °C | 2.45e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.45e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire | |
200.0 °C | 2.45e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.45e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire | |
300 °C | 2.55e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.55e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire | |
300.0 °C | 2.55e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.55e-05 1/K | O | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Wire | |
Schmelzpunkt | 660.0 °C Show Material materials with Schmelzpunkt of 660.0 °C | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | |
Spezifische Wärmekapazität | 900.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 900.0 J/(kg·K) | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | |
20.0 °C | 900.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 900.0 J/(kg·K) | O | EN 573-3 | Rod, Sheet, Strip, Wire | |
Wärmeleitfähigkeit | 232 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 232 W/(m·K) | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | |
20.0 °C | 215.0 - 227.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 215.0 - 227.0 W/(m·K) | O | EN 573-3 | Rod, Sheet, Strip, Wire |
Elektrisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Elektrische Leitfähigkeit | 37500000.0 - 37700000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 37500000.0 - 37700000.0 S/m | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | |
20.0 °C | 37600000.0 - 37800000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 37600000.0 - 37800000.0 S/m | O | EN 573-3 | Rod, Sheet, Strip, Wire | |
spezifischer Widerstand | 2.65e-08 - 2.67e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.65e-08 - 2.67e-08 Ω·m | O | EN 573-3, EN 1301 | Strip, Sheet, Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 99.98 % Show Material materials with Aluminium of 99.98 % | O | EN 573-3, EN 1301 | Rod, Sheet, Strip, Wire, Plate |
Eisen | 0.006 % Show Material materials with Eisen of 0.006 % | O | EN 573-3 | Rod, Sheet, Strip, Wire |
0.006 % Show Material materials with Eisen of 0.006 % | O | EN 573-3, EN 1301 | Strip, Sheet, Plate | |
Kupfer | 0.003 % Show Material materials with Kupfer of 0.003 % | O | EN 573-3, EN 1301 | Rod, Sheet, Strip, Wire, Plate |
Silizium | 0.01 % Show Material materials with Silizium of 0.01 % | O | EN 573-3, EN 1301 | Rod, Sheet, Strip, Wire, Plate |
Titan | 0.003 % Show Material materials with Titan of 0.003 % | O | EN 573-3, EN 1301 | Rod, Sheet, Strip, Wire, Plate |
Zink | 0.015 % Show Material materials with Zink of 0.015 % | O | EN 573-3, EN 1301 | Rod, Sheet, Strip, Wire, Plate |
Technological properties
Property | ||
---|---|---|
Brazing | hard brazing (with flux/ without flux): very good / very good, friction soldering: very good, soft brazing with flux: very good, general: very good | |
Corrosion properties | Seawater: acceptable, weathering: good | |
Workability | Bending / Spinning (cold): very good |