Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.71 g/cm³ Show Material materials with Dichte of 2.71 g/cm³ | H24 | EN 573-3, EN 683 | Strip, Sheet |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastizitätsmodul | 69.0 GPa Show Material materials with Elastizitätsmodul of 69.0 GPa | H24 | EN 573-3, EN 683 | Strip, Sheet | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | ||||
Schubmodule | 25.9 GPa Show Material materials with Schubmodule of 25.9 GPa | Typical for Wrought 1000 Series Aluminium | ||||
Zugfestigkeit | 20.0 °C | 110.0 - 160.0 MPa Show Material materials with Zugfestigkeit of 110.0 - 160.0 MPa | H24 | EN 573-3 | Foil | |
20.0 °C | 115.0 - 160.0 MPa Show Material materials with Zugfestigkeit of 115.0 - 160.0 MPa | H24 | EN 573-3, EN 683 | Strip, Sheet, Foil |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.36e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K | H24 | EN 573-3, EN 683 | Strip, Sheet | |
100 °C | 2.36e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K | H24 | EN 573-3, EN 683 | Strip, Sheet | ||
Schmelzpunkt | 640.0 - 655.0 °C Show Material materials with Schmelzpunkt of 640.0 - 655.0 °C | H24 | EN 573-3, EN 683 | Strip, Sheet | ||
Spezifische Wärmekapazität | 900.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 900.0 - 963.0 J/(kg·K) | Typical for Wrought 1000 Series Aluminium | ||||
Wärmeleitfähigkeit | 218.0 - 222.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 218.0 - 222.0 W/(m·K) | H24 | EN 573-3, EN 683 | Strip, Sheet |
Elektrisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Elektrische Leitfähigkeit | 33000000.0 - 34000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 33000000.0 - 34000000.0 S/m | H24 | EN 573-3, EN 683 | Strip, Sheet |
spezifischer Widerstand | 2.94e-08 - 3.03e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.94e-08 - 3.03e-08 Ω·m | H24 | EN 573-3, EN 683 | Strip, Sheet |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 99.0 % Show Material materials with Aluminium of 99.0 % | H24 | EN 573-3, EN 683 | Foil, Strip, Sheet |
Kupfer | 0.05 - 0.2 % Show Material materials with Kupfer of 0.05 - 0.2 % | H24 | EN 573-3, EN 683 | Foil, Strip, Sheet |
Mangan | 0.05 % Show Material materials with Mangan of 0.05 % | H24 | EN 573-3, EN 683 | Foil, Strip, Sheet |
Zink | 0.1 % Show Material materials with Zink of 0.1 % | H24 | EN 573-3, EN 683 | Foil, Strip, Sheet |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |