Das Material: 'Silver (Ag) soft annealed ( A)', nach dem Sie gesucht haben, wurde durch das untenstehende ersetzt.

Silver (Ag) 30 % cold worked

Want to keep this datasheet? Save it now in your required format

Description

Silver (Ag) is a white-shining, in very thin films blue-green translucent, in regular octahedra (cubic densest sphere packing) crystallizing metal. Ag is the most malleable metal after gold, can be pulled out to wire of 0.008 mm diameter and rolled out to the thinnest films. Silver has the highest electrical and thermal conductivity of all metals, plus the best reflectivity. Against oxygen and caustic alkalis, silver is very stable at normal and also at elevated temperature. In contrast, it has an increased affinity for sulfur. The sulfur compounds formed on silver objects blacken silver. Nitric acid dissolves it to form silver nitrate. Silver bromide decomposes under the action of light. However, it forms silver sulfide in a sulfur-containing atmosphere, which can be very disturbing for small contact forces, as they occur in the news and information technology. For larger contact forces, as they are common in power engineering, but silver sulfides do not disturb. Silver is relatively soft and is hardened in a manner similar to gold by alloying with Au, Pt, Pd, Cu, Zn, Sn, Cd, Si, Mg or Mn. With not too large proportions of the hardening metals, easily deformable alloys are obtained. Ag is also used as a coating material, it is plated on brass, copper and steel or a silver layer is electroplated (silver plating). Application: In the chemical technique for porous disks in filtration, as catalyst in catalysis. As a fusible conductor is pure silver (Ag1000) due to its aging resistance, its oxide-free surfaces and good solder wettability, its perfect contact and the fact that pure silver has a small melting integral, low heat of fusion (nimble fuses), very well suited for low-voltage and High-voltage high-performance fuses, used for power converter fuses and for miniature fuses. Silver is the most commonly used contact material, but tends to weld and has relatively high material migration. Ag is very ductile, sulfur-sensitive and oxidation-resistant up to 180 ° C. It is machinable, roll-cladable, electrodepositable and can be separated from the gas phase.

Related Standards

Diese Materialdaten wurden von WIAM zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValue

Dichte

20.0 °C

10.5 g/cm³

Show Material materials with Dichte of 10.5 g/cm³

Mechanisch

PropertyTemperatureValueComment

Elastizitätsmodul

-195.0 °C

89 GPa

Show Material materials with Elastizitätsmodul of 89 GPa

20.0 °C

80 GPa

Show Material materials with Elastizitätsmodul of 80 GPa

200.0 °C

77 GPa

Show Material materials with Elastizitätsmodul of 77 GPa

400.0 °C

67 GPa

Show Material materials with Elastizitätsmodul of 67 GPa

600.0 °C

57 GPa

Show Material materials with Elastizitätsmodul of 57 GPa

800.0 °C

46 GPa

Show Material materials with Elastizitätsmodul of 46 GPa

900.0 °C

40 GPa

Show Material materials with Elastizitätsmodul of 40 GPa

Härte, Vickers

20.0 °C

70 [-]

Show Material materials with Härte, Vickers of 70 [-]

Poissonzahl

23.0 °C

0.37 [-]

Show Material materials with Poissonzahl of 0.37 [-]

Typical for Silver

Schubmodule

20.0 °C

26 GPa

Show Material materials with Schubmodule of 26 GPa

Thermisch

PropertyTemperatureValueComment

Koeffizient der thermischen Ausdehnung

100.0 °C

1.79E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.79E-5 1/K

150.0 °C

1.86E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.86E-5 1/K

200.0 °C

1.91E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.91E-5 1/K

250.0 °C

1.92E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.92E-5 1/K

300.0 °C

1.94E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.94E-5 1/K

350.0 °C

1.97E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.97E-5 1/K

400.0 °C

1.99E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.99E-5 1/K

450.0 °C

2.01E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.01E-5 1/K

500.0 °C

2.04E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.04E-5 1/K

600.0 °C

2.12E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.12E-5 1/K

700.0 °C

2.25E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.25E-5 1/K

800.0 °C

2.36E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36E-5 1/K

900.0 °C

2.43E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.43E-5 1/K

Unlock all property charts

Schmelzpunkt

962 °C

Show Material materials with Schmelzpunkt of 962 °C

Typical for Silver

Spezifische Wärmekapazität

23.0 °C

234 - 251 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 234 - 251 J/(kg·K)

Typical for Silver

Wärmeleitfähigkeit

-233.0 °C

1050 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 1050 W/(m·K)

-173.0 °C

475 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 475 W/(m·K)

-73.0 °C

441 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 441 W/(m·K)

20.0 °C

419 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 419 W/(m·K)

127.0 °C

426 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 426 W/(m·K)

327.0 °C

411 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 411 W/(m·K)

527.0 °C

397 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 397 W/(m·K)

927.0 °C

383 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 383 W/(m·K)

Unlock all property charts

Elektrisch

PropertyTemperatureValue

Elektrische Leitfähigkeit

20.0 °C

6.00E+7 S/m

Show Material materials with Elektrische Leitfähigkeit of 6.00E+7 S/m

spezifischer Widerstand

20.0 °C

1.67E-8 - 1.8E-8 Ω·m

Show Material materials with spezifischer Widerstand of 1.67E-8 - 1.8E-8 Ω·m

Chemical properties

PropertyValue

Silber

99.97 %

Show Material materials with Silber of 99.97 %