Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 16 g/cm³ Show Material materials with Dichte of 16 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 83 GPa Show Material materials with Elastizitätsmodul of 83 GPa | Typical for Silver |
Härte, Vickers | 20.0 °C | 180 [-] Show Material materials with Härte, Vickers of 180 [-] | |
Poissonzahl | 23.0 °C | 0.37 [-] Show Material materials with Poissonzahl of 0.37 [-] | Typical for Silver |
Schubmodule | 23.0 °C | 30 GPa Show Material materials with Schubmodule of 30 GPa | Typical for Silver |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.9E-5 1/K | Typical for Silver |
Schmelzpunkt | 962 °C Show Material materials with Schmelzpunkt of 962 °C | Typical for Silver | |
Spezifische Wärmekapazität | 23.0 °C | 234 - 251 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 234 - 251 J/(kg·K) | Typical for Silver |
Wärmeleitfähigkeit | 20.0 °C | 239 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 239 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 2.20E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 2.20E+7 S/m |
spezifischer Widerstand | 20.0 °C | 4.6E-8 Ω·m Show Material materials with spezifischer Widerstand of 4.6E-8 Ω·m |