Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Vickers, 5 | 20.0 °C | 95 [-] Show Material materials with Härte, Vickers, 5 of 95 [-] |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 1040 °C Show Material materials with Schmelzpunkt of 1040 °C |
Chemical properties
Property | Value |
---|---|
Gold | 75.7 % Show Material materials with Gold of 75.7 % |
Kupfer | 4.1 % Show Material materials with Kupfer of 4.1 % |
Palladium | 3.3 % Show Material materials with Palladium of 3.3 % |
Platin | 2 % Show Material materials with Platin of 2 % |
Silber | 15 % Show Material materials with Silber of 15 % |
Zink | 2 % Show Material materials with Zink of 2 % |