Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 11.4 g/cm³ Show Material materials with Dichte of 11.4 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 2 % Show Material materials with Dehnung of 2 % | |
Elastizitätsmodul | 20.0 °C | 135 GPa Show Material materials with Elastizitätsmodul of 135 GPa | |
Härte, Vickers | 20.0 °C | 205 [-] Show Material materials with Härte, Vickers of 205 [-] | |
Poissonzahl | 23.0 °C | 0.39 [-] Show Material materials with Poissonzahl of 0.39 [-] | Typical for Palladium |
Schubmodule | 20.0 °C | 47 GPa Show Material materials with Schubmodule of 47 GPa | |
Streckgrenze Rp 0,2 | 20.0 °C | 690 MPa Show Material materials with Streckgrenze Rp 0,2 of 690 MPa | |
Zugfestigkeit | 20.0 °C | 700 MPa Show Material materials with Zugfestigkeit of 700 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 300.0 °C | 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-5 1/K | |
Schmelzpunkt | 1553 °C Show Material materials with Schmelzpunkt of 1553 °C | Typical for Palladium | |
Spezifische Wärmekapazität | 23.0 °C | 236 - 248 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 236 - 248 J/(kg·K) | Typical for Palladium |
Wärmeleitfähigkeit | 23.0 °C | 60 - 76 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 60 - 76 W/(m·K) | Typical for Palladium |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 4.13E-7 Ω·m Show Material materials with spezifischer Widerstand of 4.13E-7 Ω·m |