Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 11.1 g/cm³ Show Material materials with Dichte of 11.1 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 121 GPa Show Material materials with Elastizitätsmodul of 121 GPa | Typical for Palladium |
Härte, Vickers | 20.0 °C | 90 [-] Show Material materials with Härte, Vickers of 90 [-] | |
Poissonzahl | 23.0 °C | 0.39 [-] Show Material materials with Poissonzahl of 0.39 [-] | Typical for Palladium |
Schubmodule | 23.0 °C | 42 GPa Show Material materials with Schubmodule of 42 GPa | Typical for Palladium |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.1E-5 - 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-5 - 1.4E-5 1/K | Typical for Palladium |
Schmelzpunkt | 1553 °C Show Material materials with Schmelzpunkt of 1553 °C | Typical for Palladium | |
Spezifische Wärmekapazität | 23.0 °C | 236 - 248 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 236 - 248 J/(kg·K) | Typical for Palladium |
Wärmeleitfähigkeit | 23.0 °C | 60 - 76 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 60 - 76 W/(m·K) | Typical for Palladium |