Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 19.3 g/cm³ Show Material materials with Dichte of 19.3 g/cm³ | Typical for Gold |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 74 - 81 GPa Show Material materials with Elastizitätsmodul of 74 - 81 GPa | Typical for Gold |
Härte, Vickers, 5 | 20.0 °C | 235 [-] Show Material materials with Härte, Vickers, 5 of 235 [-] | |
Poissonzahl | 23.0 °C | 0.42 [-] Show Material materials with Poissonzahl of 0.42 [-] | Typical for Gold |
Schubmodule | 23.0 °C | 26 GPa Show Material materials with Schubmodule of 26 GPa | Typical for Gold |
Streckgrenze Rp 0,2 | 20.0 °C | 620 MPa Show Material materials with Streckgrenze Rp 0,2 of 620 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-5 1/K | Typical for Gold |
Schmelzpunkt | 1064 °C Show Material materials with Schmelzpunkt of 1064 °C | Typical for Gold | |
Spezifische Wärmekapazität | 23.0 °C | 126 - 138 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 126 - 138 J/(kg·K) | Typical for Gold |
Wärmeleitfähigkeit | 23.0 °C | 292 - 316 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 292 - 316 W/(m·K) | Typical for Gold |
Chemical properties
Property | Value |
---|---|
Gold | 70 % Show Material materials with Gold of 70 % |
Kupfer | 8.8 % Show Material materials with Kupfer of 8.8 % |
Palladium | 2 % Show Material materials with Palladium of 2 % |
Platin | 4.4 % Show Material materials with Platin of 4.4 % |
Silber | 13.5 % Show Material materials with Silber of 13.5 % |
Zink | 2 % Show Material materials with Zink of 2 % |