Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 21.6 g/cm³ Show Material materials with Dichte of 21.6 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 20.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | |
Härte, Vickers | 20.0 °C | 170 [-] Show Material materials with Härte, Vickers of 170 [-] | |
Poissonzahl | 23.0 °C | 0.39 [-] Show Material materials with Poissonzahl of 0.39 [-] | Typical for Platinum |
Schubmodule | 23.0 °C | 62 GPa Show Material materials with Schubmodule of 62 GPa | Typical for Platinum |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8.8E-6 - 9.1E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.8E-6 - 9.1E-6 1/K | Typical for Platinum |
Schmelzpunkt | 1769 °C Show Material materials with Schmelzpunkt of 1769 °C | Typical for Platinum | |
Spezifische Wärmekapazität | 23.0 °C | 136 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 136 J/(kg·K) | Typical for Platinum |
Wärmeleitfähigkeit | 20.0 °C | 29 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 29 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 4.50E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 4.50E+6 S/m |
spezifischer Widerstand | 20.0 °C | 2.22E-7 Ω·m Show Material materials with spezifischer Widerstand of 2.22E-7 Ω·m |