Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 21.5 g/cm³ Show Material materials with Dichte of 21.5 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 2 % Show Material materials with Dehnung of 2 % | |
Elastizitätsmodul | 20.0 °C | 190 GPa Show Material materials with Elastizitätsmodul of 190 GPa | |
Härte, Vickers | 20.0 °C | 154 [-] Show Material materials with Härte, Vickers of 154 [-] | |
Poissonzahl | 23.0 °C | 0.39 [-] Show Material materials with Poissonzahl of 0.39 [-] | Typical for Platinum |
Schubmodule | 23.0 °C | 62 GPa Show Material materials with Schubmodule of 62 GPa | Typical for Platinum |
Streckgrenze Rp 0,2 | 20.0 °C | 450 MPa Show Material materials with Streckgrenze Rp 0,2 of 450 MPa | |
Zugfestigkeit | 20.0 °C | 470 MPa Show Material materials with Zugfestigkeit of 470 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8.8E-6 - 9.1E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.8E-6 - 9.1E-6 1/K | Typical for Platinum |
Schmelzpunkt | 1769 °C Show Material materials with Schmelzpunkt of 1769 °C | Typical for Platinum | |
Spezifische Wärmekapazität | 23.0 °C | 136 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 136 J/(kg·K) | Typical for Platinum |
Wärmeleitfähigkeit | 20.0 °C | 42 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 42 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 5.60E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 5.60E+6 S/m |
spezifischer Widerstand | 20.0 °C | 1.79E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.79E-7 Ω·m |