Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 19.2 g/cm³ Show Material materials with Dichte of 19.2 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 21 % Show Material materials with Dehnung of 21 % | |
Elastizitätsmodul | 20.0 °C | 184 GPa Show Material materials with Elastizitätsmodul of 184 GPa | |
Härte, Vickers | 20.0 °C | 210 [-] Show Material materials with Härte, Vickers of 210 [-] | |
Poissonzahl | 23.0 °C | 0.39 [-] Show Material materials with Poissonzahl of 0.39 [-] | Typical for Platinum |
Schubmodule | 20.0 °C | 73 GPa Show Material materials with Schubmodule of 73 GPa | |
Streckgrenze Rp 0,2 | 20.0 °C | 460 MPa Show Material materials with Streckgrenze Rp 0,2 of 460 MPa | |
Zugfestigkeit | 20.0 °C | 620 MPa Show Material materials with Zugfestigkeit of 620 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 300.0 °C | 1.04E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.04E-5 1/K | |
Schmelzpunkt | 1769 °C Show Material materials with Schmelzpunkt of 1769 °C | Typical for Platinum | |
Spezifische Wärmekapazität | 23.0 °C | 136 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 136 J/(kg·K) | Typical for Platinum |
Wärmeleitfähigkeit | 23.0 °C | 69 - 73 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 69 - 73 W/(m·K) | Typical for Platinum |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 2.7E-7 Ω·m Show Material materials with spezifischer Widerstand of 2.7E-7 Ω·m |