Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 20 g/cm³ Show Material materials with Dichte of 20 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 32 % Show Material materials with Dehnung of 32 % | |
Elastizitätsmodul | 20.0 °C | 208 GPa Show Material materials with Elastizitätsmodul of 208 GPa | |
Härte, Vickers | 20.0 °C | 102 [-] Show Material materials with Härte, Vickers of 102 [-] | |
Poissonzahl | 23.0 °C | 0.39 [-] Show Material materials with Poissonzahl of 0.39 [-] | Typical for Platinum |
Schubmodule | 20.0 °C | 72 GPa Show Material materials with Schubmodule of 72 GPa | |
Streckgrenze | 20.0 °C | 180 MPa Show Material materials with Streckgrenze of 180 MPa | |
Streckgrenze Rp 0,2 | 20.0 °C | 180 MPa Show Material materials with Streckgrenze Rp 0,2 of 180 MPa | |
Zugfestigkeit | 20.0 °C | 300 MPa Show Material materials with Zugfestigkeit of 300 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 300.0 °C | 1.02E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.02E-5 1/K | |
700.0 °C | 1.07E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.07E-5 1/K | ||
1200.0 °C | 1.12E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.12E-5 1/K | ||
Schmelzpunkt | 1769 °C Show Material materials with Schmelzpunkt of 1769 °C | Typical for Platinum | |
Spezifische Wärmekapazität | 23.0 °C | 136 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 136 J/(kg·K) | Typical for Platinum |
Wärmeleitfähigkeit | 20.0 °C | 30 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 30 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 2E-7 Ω·m Show Material materials with spezifischer Widerstand of 2E-7 Ω·m |
Chemical properties