Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 21.4 g/cm³ Show Material materials with Dichte of 21.4 g/cm³ | Typical for Platinum |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 44 % Show Material materials with Dehnung of 44 % | |
200.0 °C | 40 % Show Material materials with Dehnung of 40 % | ||
300.0 °C | 37 % Show Material materials with Dehnung of 37 % | ||
400.0 °C | 40 % Show Material materials with Dehnung of 40 % | ||
500.0 °C | 42 % Show Material materials with Dehnung of 42 % | ||
600.0 °C | 44 % Show Material materials with Dehnung of 44 % | ||
700.0 °C | 46 % Show Material materials with Dehnung of 46 % | ||
900.0 °C | 56 % Show Material materials with Dehnung of 56 % | ||
1100.0 °C | 63 % Show Material materials with Dehnung of 63 % | ||
1250.0 °C | 71 % Show Material materials with Dehnung of 71 % | ||
1500.0 °C | 67 % Show Material materials with Dehnung of 67 % | ||
Elastizitätsmodul | 23.0 °C | 154 - 172 GPa Show Material materials with Elastizitätsmodul of 154 - 172 GPa | Typical for Platinum |
Flächenreduzierung | 20.0 °C | 98 % Show Material materials with Flächenreduzierung of 98 % | |
300.0 °C | 98 % Show Material materials with Flächenreduzierung of 98 % | ||
500.0 °C | 98 % Show Material materials with Flächenreduzierung of 98 % | ||
700.0 °C | 98 % Show Material materials with Flächenreduzierung of 98 % | ||
900.0 °C | 98 % Show Material materials with Flächenreduzierung of 98 % | ||
1100.0 °C | 94 % Show Material materials with Flächenreduzierung of 94 % | ||
1250.0 °C | 99 % Show Material materials with Flächenreduzierung of 99 % | ||
1500.0 °C | 99 % Show Material materials with Flächenreduzierung of 99 % | ||
Poissonzahl | 23.0 °C | 0.39 [-] Show Material materials with Poissonzahl of 0.39 [-] | Typical for Platinum |
Schubmodule | 23.0 °C | 62 GPa Show Material materials with Schubmodule of 62 GPa | Typical for Platinum |
Zugfestigkeit | 20.0 °C | 221 - 225 MPa Show Material materials with Zugfestigkeit of 221 - 225 MPa | |
200.0 °C | 190 MPa Show Material materials with Zugfestigkeit of 190 MPa | ||
300.0 °C | 170 MPa Show Material materials with Zugfestigkeit of 170 MPa | ||
400.0 °C | 150 MPa Show Material materials with Zugfestigkeit of 150 MPa | ||
500.0 °C | 135 - 138 MPa Show Material materials with Zugfestigkeit of 135 - 138 MPa | ||
600.0 °C | 120 MPa Show Material materials with Zugfestigkeit of 120 MPa | ||
700.0 °C | 101 - 103 MPa Show Material materials with Zugfestigkeit of 101 - 103 MPa | ||
900.0 °C | 70 MPa Show Material materials with Zugfestigkeit of 70 MPa | ||
1100.0 °C | 42 MPa Show Material materials with Zugfestigkeit of 42 MPa | ||
1250.0 °C | 30 MPa Show Material materials with Zugfestigkeit of 30 MPa | ||
1500.0 °C | 16 MPa Show Material materials with Zugfestigkeit of 16 MPa | ||
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8.8E-6 - 9.1E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.8E-6 - 9.1E-6 1/K | Typical for Platinum |
Schmelzpunkt | 1769 °C Show Material materials with Schmelzpunkt of 1769 °C | Typical for Platinum | |
Spezifische Wärmekapazität | 23.0 °C | 136 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 136 J/(kg·K) | Typical for Platinum |
Wärmeleitfähigkeit | 20.0 °C | 33 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 33 W/(m·K) |
Chemical properties