Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 21.4 g/cm³ Show Material materials with Dichte of 21.4 g/cm³ | Typical for Platinum |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 24 % Show Material materials with Dehnung of 24 % | |
Elastizitätsmodul | 20.0 °C | 204 GPa Show Material materials with Elastizitätsmodul of 204 GPa | |
Härte, Vickers | 20.0 °C | 139 [-] Show Material materials with Härte, Vickers of 139 [-] | |
Poissonzahl | 23.0 °C | 0.39 [-] Show Material materials with Poissonzahl of 0.39 [-] | Typical for Platinum |
Schubmodule | 23.0 °C | 62 GPa Show Material materials with Schubmodule of 62 GPa | Typical for Platinum |
Streckgrenze Rp 0,2 | 20.0 °C | 270 MPa Show Material materials with Streckgrenze Rp 0,2 of 270 MPa | |
Zugfestigkeit | 20.0 °C | 450 MPa Show Material materials with Zugfestigkeit of 450 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8.8E-6 - 9.1E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.8E-6 - 9.1E-6 1/K | Typical for Platinum |
Schmelzpunkt | 1769 °C Show Material materials with Schmelzpunkt of 1769 °C | Typical for Platinum | |
Spezifische Wärmekapazität | 23.0 °C | 136 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 136 J/(kg·K) | Typical for Platinum |
Wärmeleitfähigkeit | 23.0 °C | 69 - 73 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 69 - 73 W/(m·K) | Typical for Platinum |