Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.19 g/cm³ Show Material materials with Dichte of 7.19 g/cm³ | Typical for Chromium |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 279 GPa Show Material materials with Elastizitätsmodul of 279 GPa | Typical for Chromium |
Poissonzahl | 23.0 °C | 0.21 [-] Show Material materials with Poissonzahl of 0.21 [-] | Typical for Chromium |
Schubmodule | 23.0 °C | 115 GPa Show Material materials with Schubmodule of 115 GPa | Typical for Chromium |
Streckgrenze | 20.0 °C | 590 MPa Show Material materials with Streckgrenze of 590 MPa | |
Zugfestigkeit | 20.0 °C | 760 MPa Show Material materials with Zugfestigkeit of 760 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4.9E-6 - 8.2E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 4.9E-6 - 8.2E-6 1/K | Typical for Chromium |
Schmelzpunkt | 1875 °C Show Material materials with Schmelzpunkt of 1875 °C | Typical for Chromium | |
Spezifische Wärmekapazität | 23.0 °C | 442 - 487 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 442 - 487 J/(kg·K) | Typical for Chromium |
Wärmeleitfähigkeit | 23.0 °C | 87 - 91 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 87 - 91 W/(m·K) | Typical for Chromium |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.25 % Show Material materials with Aluminium of 0.25 % |
Chrom | 58 - 62 % Show Material materials with Chrom of 58 - 62 % |
Eisen | 1 % Show Material materials with Eisen of 1 % |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % |
Mangan | 0.3 % Show Material materials with Mangan of 0.3 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Stickstoff | 0.3 % Show Material materials with Stickstoff of 0.3 % |
Titan | 0.5 % Show Material materials with Titan of 0.5 % |